Lead Telluride - PbTe

Classification: Telluride
Atomic numbers: 82 & 52
Atomic weight: 334.79
Melting point (C): >700
Boiling point (C):
Density (g/cm3): 8.16
Refractive index (n=):
Hardness (Mosh-scratch): 3
Crystal structure: Isometric-normal: (100) cube
Color (solid): Tin-white/yellowish
Cleavage: (100)