Lithium Nitride - Li3N

Classification: Nitride
Atomic numbers: 3 & 7
Atomic weight: 34.83
Melting point (C): 845
Boiling point (C):
Density (g/cm3):
Refractive index (n=):
Hardness (Mosh-scratch): 5-6
Crystal structure: Isometric-normal: (100) cube
Color (solid): Solid-crystalline: Grey/black, solid/amorphous: Red-brown
Cleavage: Cubic: (001)