Magnesium Nitride - Mg3N2

Classification: Nitride
Atomic numbers: 12 & 7
Atomic weight: 100.98
Melting point (C): 1500
Boiling point (C):
Density (g/cm3): 2.xx
Refractive index (n=):
Hardness (Mosh-scratch): 7-8
Crystal structure: Monoclinc-normal: (100) a pinacoid
Color (solid): Colorless
Cleavage: Basal: (001)