Radon

Symbol: Rn
Atomic Number: 86
Atomic Weight: 222.0176
Element Classification: Inert Gas
Discovered By: Fredrich Ernst Dorn
Discovery Date: 1898 (Germany)
Name Origin: Variation of the name of another element, radium.

Density (g/cc): 4.4 (@ -62C)
Melting Point (K): 202
Boiling Point (K): 211.4
Appearance: Heavy radioactive gas
Atomic Radius (pm): n/a
Atomic Volume (cc/mol): n/a
Covalent Radius (pm): n/a
Ionic Radius: n/a
Specific Heat (@20C J/g mol): 0.094
Fusion Heat (kJ/mol): n/a
Evaporation Heat (kJ/mol): 18.1
Thermal Conductivity (@25C W/m K):
Debye Temperature (K): n/a
Pauling Negativity Number: n/a
First Ionizing Energy (kJ/mol): 1036.5
Oxidation States: n/a
Electronic Configuration: [Xe] 4f14 5d10 6s2 6p6
Lattice Structure: Face-Centered Cubic (FCC)
Lattice Constant (): n/a
Lattice C/A Ratio: n/a