ASTM Electrolytes for Electropolishing

3% Si-Fe specimen - Electrolytic polishing
Ag3Ni specimens - Electrolytic polishing
Al and Al alloys - Electrolytic polishing
Al and Al alloys - Electrolytic polishing
Al and Al alloys with less than 2% Si - Electrolytic polishing
Al, Al-Si alloys - Electrolytic polishing
Al-Mg alloys - Electrolytic polishing
Al-Si alloys - Electrolytic polishing
Alloy steels - Electrolytic polishing
Alloy steels - Electrolytic polishing
Alloy steels - Electrolytic polishing
Alpha or alpha plus beta brass - Electrolytic polishing
Aluminium - Electrolytic polishing
Aluminium - Electrolytic polishing
Aluminium - Electrolytic polishing
Aluminium - Electrolytic polishing
Aluminium - Electrolytic polishing
Aluminium - Electrolytic polishing
Aluminium - Electrolytic polishing
Antimony specimens - Electrolytic polishing
Antimony specimens - Electrolytic polishing
Beryllium - Electrolytic polishing
Beryllium - Electrolytic polishing
Bismuth - Electrolytic polishing
Bismuth - Electrolytic polishing
Bismuth - Electrolytic polishing
Brass specimens - Electrolytic polishing
Brass specimens - Electrolytic polishing
Brass specimens - Electrolytic polishing
Bronze (up to 6% Sn) - Electrolytic polishing
Bronze (up to 9% Sn) - Electrolytic polishing
Cadmium - Electrolytic polishing
Cadmium - Electrolytic polishing
Carbon steels - Electrolytic polishing
Carbon steels - Electrolytic polishing
Cast iron specimens - Electrolytic polishing
Chromium - Electrolytic polishing
Chromium - Electrolytic polishing
Chromium - Good general-purpose elctrolyte
Cobalt and alloys - Electrolytic polishing
Cobalt and alloys - Electrolytic polishing
Copper - Electrolytic polishing
Copper - Electrolytic polishing
Copper alloys - Electrolytic polishing
Cu and Cu alloys except Sn bronze - Electrolytic polishing
Cu and Cu-base alloys - Electrolytic polishing
Cu-Fe, Cu-Co alloys - Electrolytic polishing
Cu-Pb alloys - Good up to 30% Pb
Cu-Zn alloy - Electrolytic polishing
Germanium - Electrolytic polishing
Germanium - Electrolytic polishing
Gold - Electrolytic polishing
Hafnium - Used to polish Hf wires
Heat resisting alloys - Electrolytic polishing
High speed steels - Electrolytic polishing
High-temperature alloys - Electrolytic polishing
Iron specimen - Electrolytic polishing
Iron specimen - Electrolytic polishing
Iron specimen - Electrolytic polishing
Iron specimen - Electrolytic polishing
Lead - Electrolytic polishing
Lead - Electrolytic polishing
Lead - Electrolytic polishing
Magnesium - Electrolytic polishing
Mg and high Mg alloys - Electrolytic polishing
Mg-Zn alloy - Electrolytic polishing
Mn, Mn-Cu alloys - Electrolytic polishing
Mo and Mo alloys - Electrolytic polishing
Molybdenum - Electrolytic polishing
Molybdenum - Electrolytic polishing
Molybdenum - Electrolytic polishing
Molybdenum - Electrolytic polishing
Molybdenum - Particulary good for sintered Mo-32 to 80 F
Molybdenum, sintered and cast - Electrolytic polishing
Monel - Electrolytic polishing
Neptunium - Electrolytic polishing
Ni-Chrome - Electrolytic polishing
Ni-base superalloy - Electrolytic polishing
Ni-base superalloys - Electrolytic polishing
Nickel - Electrolytic polishing
Nickel - Electrolytic polishing
Nickel - Electrolytic polishing
Nickel - Electrolytic polishing
Nickel - Electrolytic polishing
Nickel - Electrolytic polishing
Nickel - Electrolytic polishing
Niobium - Electrolytic polishing
Niobium - Electrolytic polishing
Pb, Pb-Sn, Pb-Sn-Cd, Pb-Sn-Sb - Electrolytic polishing
Pb-Sn alloys - Electrolytic polishing
Pure Zinc - Electrolytic polishing
Pure copper - Electrolytic polishing
Silver - Electrolytic polishing
Silver - Electrolytic polishing
Silver - Electrolytic polishing
Silver - Electrolytic polishing
Silver - Electrolytic polishing
Stainless steel - Electrolytic polishing
Stainless steel - Electrolytic polishing
Stainless steel - Electrolytic polishing
Stainless steel - Electrolytic polishing
Stainless steel - Electrolytic polishing
Stainless steel - Electrolytic polishing
Stainless steel - Electrolytic polishing
Stainless steel - Electrolytic polishing
Stainless steel - Electrolytic polishing
Stainless steel - Electrolytic polishing
Stainless steel - Electrolytic polishing
Stainless steel - Electrolytic polishing
Stainless steel - Electrolytic polishing
Stainless steel - Electrolytic polishing
Stainless steel - Electrolytic polishing
Stainless steel - Electrolytic polishing
Stainless steel - Electrolytic polishing
Stainless steel - Electrolytic polishing
Stainless steel - Electrolytic polishing
Stainless steel - Electrolytic polishing
Stainless steel - Electrolytic polishing
Stainless steel - Electrolytic polishing
Stainless steel - Good for all austenitic heat resistant alloys, 100F plus
Stainless steel and alloy steel - Electrolytic polishing
Stainless steel and alloy steel - Electrolytic polishing
Stainlesss steels - Electrolytic polishing
Steel - Carbon and alloy - Electrolytic polishing
Steel - Carbon, alloy, stainless - Electrolytic polishing
Steel carbon and alloy - Electrolytic polishing
Steel carbon and alloy - Electrolytic polishing
Steel specimens - Electrolytic polishing
Steel specimens - Electrolytic polishing
Steel specimens - Electrolytic polishing
Steel specimens - Electrolytic polishing
Tantalum - Electrolytic polishing
Tin - Electrolytic polishing
Tin - Electrolytic polishing
Tin - Electrolytic polishing
Titanium - Electrolytic polishing
Titanium - Electrolytic polishing
Titanium - Electrolytic polishing
Titanium - Electrolytic polishing
Titanium - Electrolytic polishing
Titanium - Electrolytic polishing
Titanium - Electrolytic polishing
Titanium - Electrolytic polishing
Titanium - Electrolytic polishing
Tungsten - Electrolytic polishing
Tungsten - Electrolytic polishing
U-Zr alloy - Electrolytic polishing
Uranium - Electrolytic polishing
Uranium - Electrolytic polishing
Uranium - Electrolytic polishing
Uranium - Electrolytic polishing
Uranium - Electrolytic polishing
Uranium - Electrolytic polishing
Uranium - Electrolytic polishing
Vanadium - Electrolytic polishing
Zinc - Electrolytic polishing
Zinc - Electrolytic polishing
Zinc - Electrolytic polishing
Zinc - Electrolytic polishing
Zirconium - Electrolytic polishing
Zirconium - Electrolytic polishing
Zirconium - Electrolytic polishing
Zirconium - Electrolytic polishing
Zirconium - Electrolytic polishing
Zirconium - Electrolytic polishing
Zirconium - Electrolytic polishing
Zirconium - Polish and etch simultaneously - Electrolytic polishing
Zn, Zn-Sn-Fe, Zn-Al-Cu - Electrolytic polishing