Etchants for Barium

Ba specimen - A general removal and polish etch for barium
Ba specimen - This and other single acids can be used as general etchants for barium
Ba-Zr-S system (BaZrS3) - Chemical etching - General microstructure
Ba2Si2TiO2 single crystal - Chemical etching - General microstructure
Ba2TiO3 polycrystalline hemispheres - Cut, forming
Ba2TiO3 single crystal - Thermal processing
Ba2TiO3 specimens - Chemical polishing
BaF2 (111) specimen - Gas cleaning
BaF2 (111) wafers - Acid, float-off
BaF2 (111) wafers - Chemical polishing
BaF2 (111) wafers - Chemical polishing
BaF2 specimens - Chemical etching - General microstructure
BaF3 (111) wafers - Chemical etching - General microstructure
BaO in BaTi3O7, grain boundary etchant - Physical etching - General microstructure
BaSO4 - Chemical etching - General microstructure
BaTiO3 - Chemical etching - General microstructure
BaTiO3 - Dislocation etching
BaTiO3 and BaSrTiO3 - Chemical etching - General microstructure
BaTiO3 and BaTi3O7 - Chemical etching
BaTiO3 specimens - Chemical etching - General microstructure
BaWO4 single crystal - Chemical polishing
Barium chloride (fluoride) - Chemical etching - General microstructure
Barium sulphate - Chemical polishing
Barium - Electrolytic polishing
Barium Magnesium titanate - Bax-Ti(8-x)-Mgx-O16, 1.14>x>0.6
Barium Sodium Niobate - This gives square etch pits with sides parallel to [110]T
Barium fluoride (BaF2) - Chemical etching - General microstructure
Barium fluoride (BaF2) - Chemical polishing
Barium fluoride (BaF2) - Physical etching - General microstructure
Barium fluoride single crystal (BaF2) - Chemical etching - General microstructure
Barium oxide (BaO) - Chemical etching - General microstructure
Barium oxide (BaO) - Chemical etching - General microstructure
Barium silicate (3BaO x 5SiO2) - Chemical etching - General microstructure
Barium titanate (Samarium doped) - Chemical etching - General microstructure
Barium titanate - Also used for La, Ne and Sc doped material
Barium titanate - BaTiO3, BaTi3O7 - General microstructure
Barium titanate - Chemical etching
Barium titanate - Chemical etching - General microstructure
Barium titanate - Chemical polishing
Barium-lead-titanate-zirconate - (Pb0.7Ba0.3) x (Zr0.7TiO.3)3
Iodine A etchant - Ba2TiO3 (111) and (100) wafers, single crystals - Chemical etching
Oxide ceramics - BaTiO3, BaTi3O7 - General microstructure