Fluoride Etchants

BaF2 (111) wafers - Chemical polishing
Barium chloride (fluoride) - Chemical etching
Barium Sodium Niobate - This gives square etch pits with sides parallel to [110]T
Barium fluoride (BaF2) - Chemical etching
Barium fluoride (BaF2) - Chemical polishing
Barium fluoride (BaF2) - Physical etching
Barium fluoride single crystal (BaF2) - Chemical etching
Calcium fluoride (CaF2) - Chemical etching
Calcium fluoride (CaF2) - Chemical etching
Calcium fluoride (CaF2) - Etch pit etch
Calcium fluoride (CaF2) - Etching for etch pits
Calcium fluoride (CaF2) - Final chemical polishing
Calcium fluoride (CaF2) - Jet chemical thinning
Calcium fluoride (CaF2) - Thermal etching
Calcium fluoride (CaF2) - This etchant produce etch pits parallel to <111> cleavage planes
Calcium fluoride (CaF2) - This will produce etch pits
F etchant - LiF - Dislocation etching
Li fluoride - Chemical polishing
LiF (100) wafers - Chemical etching
Lithium fluoride (LiF) - Chemical polishing
Lithium fluoride (LiF) - Chemical polishing
Lithium fluoride (LiF) - Chemical polishing
Lithium fluoride (LiF) - Chemical polishing
Lithium fluoride (LiF) - For etch pits etching
Lithium fluoride (LiF) - For etch pits etching
Lithium fluoride (LiF) single crystal - Chemical etching
Lithium fluoride (LiF) single crystal - Chemical etching
Lithium fluoride (LiF) single crystal - Chemical etching
MA 956E alloy - Fe-19Cr-4.4Al-0.5Ti-0.4Ni-0.5Y2O3
Magnesium fluoride MgF2 - Chemical polishing
Magnesium fluoride MgF2 - For etching grains in hot pressed magnesium fluoride
Sodium fluoride (NaF) - Chemical etching
Sodium fluoride (NaF) - Chemical etching
SrF2 and Ba(x)Sr(1-x)F2 thin films and SrF2 (100) wafers - Chemical etching
Steels specimen - Cast irons, steels, tool steels, manganese steels, ferritic and martensitic stainless steels
Strontium fluoride single crystal (SrF2) - Etch pits on (111) faces are revealed by etching

Copyright © 2019 by Steel Data. All Rights Reserved.