Etchants for Gadolinium and Alloys

ASTM etchant No. 55 - Gadolinium - Chemical etching
ASTM etchant No. 56 - Gadolinium - Chemical etching
ASTM etchant No. 57 - Acetic acid/peroxide - For Gd
ASTM etchant No. 57 - Gadolinium - Chemical etching
Gadolinium - Chemical etching - General microstructure
Gadolinium - Chemical polishing and etching
Gadolinium - Electrolytic polishing
Gadolinium - Pure Gd, Rare Earths - Co alloys - Grain boundary etch
Gadolinium molybdate (Beta-Gd2(MoO4)3) - Chemical etching - General microstructure
Gadolinium molybdate (Gd-Mo-O) - Etch pits etching
Gadolinium molybdate (Gd2(MoO4)3) - For revealing the antiphase boundaries
Gadolinium telluride (GdTe) - Chemical etching - General microstructure
Gd single crystal specimens - Thermal etching
Gd-Ag alloys - Chemical etching - General microstructure
Gd-Al alloy - GdAl, Gd3Al, Gd2Al - General microstructure
Gd-Bi system - Chemical etching - General microstructure
Gd-Cd alloys - Chemical etching - General microstructure
Gd-Fe alloy - Laves phase GdFe2
Gd-Ga garnet - Gd3Ga5O12
Gd-Ga garnet - Gd3Ga5O12
Gd-Ga garnets - Chemical polishing
Gd-Yb alloys - Electrolytic polishing
Gd3Ga5O12 (0001) wafers 3" in diameter - Ketone cleaning
Gd3Ga5O12 (110) wafers - Abrasive polishing
Gd3Ga5O12 (111) cut wafers - Chemical cleaning
Gd3Ga5O12 (111) wafers - Abrasive polishing
Gd3Ga5O12 garnet - Chemical etching
Gd3Ga5O12 garnets - Chemical etching
Gd3Se1.8Ga3.2O12 (0001) wafers - Chemical cleaning
GdN12 specimens - Chemical etching - General microstructure
GdTbFe thin films - Chemical etching - General microstructure