Etchants for Hf and Alloys

Al-Hf alloy-Alloy with 1.8 wt.% Hf
ASTM etchant #66
ASTM etchant #67
ASTM etchant #68
ASTM etchant #69
ASTM etchant #69
ASTM etchant #70
ASTM etchant #71
ASTM etchant #72
Cain's 'B' etchant
Ceramics, carbides (Cr, Hf, V, Al)-CrC, HfC, VC, (Al, Ti)C
Cr and Hf carbides-Chemical etching
Hafnium diboride (HfB2)-Chemical etching
Hafnium diboride (HfB2)-Chemical etching
Hafnium specimens-Zicaloy-2 and Hf
Hafnium specimens-Zr and Hf and their alloys with small additional constituents
Hafnium specimens-Zr anf Hf and their alloys
Hafnium-Electrolytic polishing
Hafnium-Electropolishing
Hafnium-Electropolishing
Hafnium-Hf base alloys
Hafnium-Hf base alloys
Hafnium-Hf
Hafnium-Hf
Hafnium-Hf
Hafnium-Hf
Hafnium-Hf
Hafnium-pure and low alloy Hf and Zr for observation in polarized light
Hafnium-pure and low alloy Hf and Zr for observation in polarized light
Hafnium-Thinning for transmission electron microscopy (TEM)
Hafnium-Used to polish Hf wires
Hafnium-Used to polish Hf wires
Hafnium-Zr and Hf base alloys. Zr-Nb alloys
Hafnium-Zr and Hf base alloys. Zr-Nb alloys
Hf single crystal wafers and HfN thin films-Chemical cleaning
Hf specimens-Chemical etching
Hf specimens-Chemical etching
Hf thin films deposited on silicon wafers-Chemical etching
Hf, Zr and allloys - Cain's chemical polish and etch
Hf, Zr, and alloys
Hf, Zr, and alloys
Hf, Zr, and alloys
Hf-Al-Pa system-HfAl1.67Pd0.23
HfB2 and ZrB2
HfB2-TaB2-Chemical etching
HfB-TaB2-Chemical etching
Hf-C alloys
Hf-C alloys-Etch for detecting free hafnium
Hf-Cr alloys-Chemical etching
Hf-Cr alloys-Electro etching
Hf-Cr and Hf-V alloys
Hf-Er system-Chemical etching
Hf-Er-Sc system-Chemical etching
Hf-Ir system-Chemical and electrolytic etchant
Hf-Nb alloys (Hf rich)-Electrolytic polishing and jet electro thinning
Hf-Nb alloys-Chemical etching
Hf-Nb alloys-Chemical polishing and electrolytic polishing
Hf-Nb-B system-Chemical etching
Hf-Nb-Si system-Hf(85-x)Nb(x)Si(15); x< 45
Hf-O system-Chemical etching
Hf-O system-Hf-HfO2 section
HfO2
HfO2
Hf-Si system (Hf85Si15)-Electro thinning
Hf-Ta alloys-Chemical polishing
Hf-V alloys-Electrolytic etching
Hf-V, Hf-Cr alloys
Hf-V-Si system-Hf(85-x)V(x)Si(15); x < 37
Hf-W alloys
Hf-W eutectoid alloys - Cain's chemical polishing and etching reagent
Nb-W-Mo-Hf alloy-SU16 alloy: 11% W, 3% Mo, 3% Hf, 0.08% C
Pure Zr, pure Hf, grain constrast-Anodizing
Re-Hf alloys-Sample preparation procedure
Ta-W-Hf alloy T-111-8% W, 2% Hf. Electro polishing by twin jet
Ta-W-Hf alloy T-111-8% W, 2% Hf
W-Hf-N alloys alloys-< 3% Hf, nitrided
W-Hf-Re alloys-Chemical etching
W-Hf-Re-N alloys alloys-< 2% Hf, < 25% Re, nitrided
W-Mo-Hf-Re alloys-<% Mo, < 2% Hf, < 30% Re
W-Mo-Hf-Re-N alloys-<% Mo, < 2% Hf, < 30% Re, nitrided
W-Re-Hf-C alloys-4 at.% Re, 0.2-0.8 at.% Hf, up to 1.35 at.% C
Zirconium specimens-Pure and low alloy Hf and Zr for observation in polarized light. Zr-U, Zr-Al, Hf-Re alloys
Zirconium specimens-Zicaloy-2 and Hf
Zirconium specimens-Zr and Hf and their alloys with small additional constituents
Zirconium specimens-Zr and Hf base alloys. Zr-Nb alloys
Zirconium specimens-Zr anf Hf and their alloys with high additional alloying constituents