Etchants for Mercury and Alloys

Alpha-HgI2 single crystal specimens - Chemical polishing
Alpha-HgI2 single crystal specimens - Chemical polishing
Hg applied as a thin film - Chemical etching
Hg as a smeared surface contact - Ketone, freezing
Hg liquid frozen - Air etching
Hg liquid frozen by submersion in LN2 - Gas etching
Hg liquid frozen into solid form - Gas etching
Hg(1-x)Cd(x)Te (111) wafers - Chemical etching
Hg(1-x)Cd(x)Te single crystal - Chemical polishing
HgAg natural single crystal - Acid, removal
HgCdTe (111) thin films - Chemical etching
HgCdTe (111) wafers - Chemical polishing
HgCdTe (111) wafers and other orientations - Chemical polishing
HgCdTe single crystal ingots and wafers - Chemical etching
HgCdTe single crystal material - Chemical polishing/etching
HgCdTe single crystal wafers - Chemical polishing
HgCdTe specimens - Chemical polishing
HgCdTe thin films - Chemical etching
HgCdTe wafers - Chemical etching
HgI2 single crystals - Ketone, growth
HgO as a native oxide on mercury - Chemical etching
HgSe (111) wafers - Chemical etching
HgSe (111) wafers - Chemical etching
HgSe (111) wafers - Chemical polishing
HgSe - Dislocation etching
HgSe single crystal specimens - Chemical polishing
HgTe (111) wafers - Chemical etching
HgTe (111) wafers - Dislocation etching
HgTe - Dislocation etching
HgTe single crystal wafers - Chemical polishing
Mercury - Electrolytic polishing
Mercury alloys - Ag-Sn-Hg alloys - General microstructure
Mercury alloys - For most amalgamates - General microstructure
Mercury alloys - Hg-Sn and Hg-Sn-Cu alloys - General microstructure
Mercury selenide (HgSe) - Chemical polishing and etching
Mercury telluride (HgTe) - Chemical polishing and etching
Mercury telluride (HgTe) - Dislocation etch
Meruric iodidie (HgI2) - Chemical polishing and etching
Meruric iodidie (HgI2) - Chemical polishing and etching
Meruric iodidie (HgI2) - Etch pits etching

Copyright © 2017 by Steel Data. All Rights Reserved.