Etchants for Niobium and Alloys

ASTM etchant No. 129 - Niobium - Chemical etching
ASTM etchant No. 129 - Niobium - Chemical etching
ASTM etchant No. 158 - Niobium
ASTM etchant No. 158 - Niobium - Chemical etching
ASTM etchant No. 158 - Niobium - Chemical etching
ASTM etchant No. 159 - Niobium
ASTM etchant No. 159 - Niobium - Chemical etching
ASTM etchant No. 159 - Niobium - Chemical etching
ASTM etchant No. 160 - Niobium
ASTM etchant No. 160 - Niobium - Chemical etching
ASTM etchant No. 160 - Niobium - Chemical etching
ASTM etchant No. 160 - Niobium - Chemical etching
ASTM etchant No. 161 - Niobium
ASTM etchant No. 161 - Niobium - Chemical etching
ASTM etchant No. 161 - Niobium - Chemical etching
ASTM etchant No. 162 - Niobium
ASTM etchant No. 162 - Niobium - Chemical etching
ASTM etchant No. 162B - Niobium - Chemical etching
ASTM etchant No. 163 - Niobium
ASTM etchant No. 163 - Niobium - Chemical etching
ASTM etchant No. 163 - Niobium - Chemical etching
ASTM etchant No. 164 - Niobium
ASTM etchant No. 164 - Niobium - Chemical etching
ASTM etchant No. 164 - Niobium - Chemical etching
ASTM etchant No. 66 - Niobium - Chemical etching
ASTM etchant No. 66 - Niobium - Chemical etching
C doped Nb-Al alloy - Nb3Al + up to 0.4 at.% C
Ceramics, carbides - NbC, NbC2 - General microstructure
Ceramics, nitrides - NbN (yelow), Nb2N (light red) - General microstructure
Cermets - NbCz-NbFe-Nb - General microstructure
D43 alloy - Nb-10W-12V-0.1C
DuPont Nb etchant - Nb-Hf and Nb alloys - Chemical etching
Fluor regia etchant - Nb and alloys - Chemical etching
Nb (100) oriented single crystal cylinders - Thermal etching
Nb (100) oriented single crystal rods - Chemical polishing
Nb and 1% Zr alloys - Chemical etching
Nb and Nb alloys - Electrolytic polishing
Nb and Nb alloys - Electrolytic polishing
Nb and Nb alloys - Electrolytic polishing
Nb and Nb alloys - Electrolytic polishing
Nb and Nb alloys - Electrolytic polishing
Nb and Nb alloys - Electrolytic polishing
Nb and Nb alloys, Ta and Ta-O alloys (industrial alloys), etch figures - Chemical etching - General microstructure
Nb and alloys - Chemical etching
Nb and alloys - Chemical etching
Nb and alloys - Chemical etching
Nb and alloys - Chemical etching
Nb and alloys - Chemical etching
Nb and alloys - Chemical etching
Nb and alloys - Chemical etching
Nb and alloys - Chemical etching
Nb and alloys - Chemical etching
Nb and alloys - Electrolytic etching
Nb oxide, NbO (blue), NbO2 (blue green), Nb2O5 (red brown) - Electrolytic etching
Nb oxides - Chemical etching
Nb polycrystalline samples - Chemical polishing
Nb specimens - Chemical cleaning
Nb specimens - Chemical cleaning
Nb specimens - Chemical etching
Nb specimens - Chemical etching
Nb specimens - Chemical etching
Nb specimens - Chemical polishing
Nb specimens - Chemical polishing
Nb specimens - Electrolytic oxidation
Nb specimens - Electrolytic polishing
Nb specimens - Hydrocarbon cleaning
Nb specimens used for electroplating - Electrolytic polishing
Nb thin films evaporated on glass - Gas oxidation
Nb, Mo, W - Electrolyticlytic lapping
Nb, NbGa, Nb3Si-Anodizing
Nb, Ta - Chemical polishing
Nb, V, Ta - Chemical polishing
Nb-Al alloy - Nb3Al - General microstructure
Nb-Al alloy - Nb3Al - General microstructure
Nb-Al alloys - Chemical etching - General microstructure
Nb-Al-Ga system - Nb3Al-Nb3Ga section - General microstructure
Nb-Al-Ga-Ge system - Nb3Al.Nb3Ga-Nb3Ge section - General microstructure
Nb-Al-Ge system - Nb3Al-Nb3Ge section - General microstructure
Nb-Al-Si system - Chemical etching - General microstructure
Nb-C alloys - Chemical ecthing
Nb-Co system - Chemical etching - General microstructure
Nb-Co-Si alloys - Chemical etching - General microstructure
Nb-Cr alloys - Chemical etching - General microstructure
Nb-Ga system - Electro etching - General microstructure
Nb-Ga system - Nb3Ga - General microstructure
Nb-Ga-Ge system - Nb3Ga-Nb3Ge section
Nb-Gd alloys - Chemical etching - General microstructure
Nb-Ge alloy (Nb3Ge) - Chemical etching - General microstructure
Nb-Ge alloy (Nb3Ge) - Chemical etching - General microstructure
Nb-Ge alloy - Anodic etching
Nb-H allooys - Chemical polishing and etching
Nb-Hf alloys - Attack polishing
Nb-Hf alloys - Attack polishing
Nb-Hf-C alloy - Nb rich alloys
Nb-Ir alloys - Chemical and electrolytic etching - General microstructure
Nb-Mo alloy - Alloys with 1-8 at.% Mo
Nb-Mo alloy - Single crystal alloys
Nb-Mo-C alloys - Attack polishing
Nb-Mo-C alloys - Chemical etching - General microstructure
Nb-N alloys - Chemical etching
Nb-N system - Chemical etching - General microstructure
Nb-N system - Chemical etching - General microstructure
Nb-N system - Electrolytic etching - General microstructure
Nb-N system - Electrolytic polishing
Nb-Ni alloy (Ni60Nb40) - Electrolytic thinning
Nb-Ni alloy - Ni-Ni3Nb eutectic
Nb-O alloys - Chemical etching
Nb-Re alloys - Chemical etching
Nb-Rh alloys (<25 at.% Rh) alloys - Chemical etching
Nb-Rh alloys - Chemical and electrolytic etching - General microstructure
Nb-Rh alloys single crystal - Chemical polishing
Nb-Ru alloys - Electrolytic etching - General microstructure
Nb-Sc alloys - Chemical etching - General microstructure
Nb-Si alloy - Anodising
Nb-Sn alloy (Nb3Sn) - Chemical etching - General microstructure
Nb-Sn alloy (Nb3Sn) - Chemical etching - General microstructure
Nb-Sn alloy (Nb3Sn) - Electrolytic thinning and polishing
Nb-Sn alloy - Anodic etching, chemical etching
Nb-Sn alloy - Chemical etching - General microstructure
Nb-Sn alloy - Chemical etching - General microstructure
Nb-Sn alloys (single crystal Nb3Sn) - Chemical etching - General microstructure
Nb-Sn alloys - Chemical ecthing
Nb-Sn alloys - Chemical etching
Nb-Sn alloys - Chemical etching
Nb-Sn alloys - Electrolytic etching
Nb-Ta alloys - Chemical polishing
Nb-Tb and Nb noble metal alloys - Chemical etching
Nb-Ti alloy (20 at.% Nb) - Chemical polishing
Nb-Ti alloy (54.3 at.% Ti) - Chemical etching - General microstructure
Nb-Ti alloy - Electrolytic thinning
Nb-Ti alloys (18-40 at.% Nb) - Chemical thinning
Nb-Ti alloys - Chemical etching
Nb-V alloys - Chemical etching - General microstructure
Nb-V and Nb alloys - Chemical etching
Nb-W-Mo-Hf alloy - SU16 alloy 11% W, 3% Mo, 3% Hf, 0.08% C
Nb-W-Zr alloy (NB7-19% W, 2% Zr) - Chemical etching - General microstructure
Nb-Zn alloys - Chemical etching - General microstructure
Nb-Zr alloy (1% Zr) - Chemical etching - General microstructure
Nb-Zr alloy (15% Nb) - Electrolytic thinning
Nb-Zr alloy (16-40% Zr) - Electrolytic polishing
Nb-Zr alloy (2.5% Nb) - Chemical thinning for electron microscopy
Nb-Zr alloy (2.7% Nb) - Chemical etching - General microstructure
Nb-Zr alloy (25 at.% Zr) - Electrolytic polishing
Nb-Zr alloy (25% Zr) - Chemical etching - General microstructure
Nb-Zr alloy (up to 20% Nb) - Chemical etching - General microstructure
Nb-Zr alloy - Micro jet machinning
Nb-Zr alloy - Sample prepation
Nb-Zr alloys (Omega phase) - Chemical polishing
Nb-Zr alloys - Chemical etching
Nb-Zr alloys - Chemical etching - General microstructure
Nb-Zr alloys - Chemical etching - General microstructure
Nb-Zr alloys - Chemical etching - General microstructure
Nb-Zr alloys - Chemical polishing and etching
Nb-Zr alloys - Electrolytic etching
Nb-Zr alloys - Electrolytic etching - General microstructure
Nb-Zr and Nb-Zr-Re alloys - Chemical etching
Nb-Zr-O system (Nb rich) - Electrolytic etching - General microstructure
Nb-low carbon alloys - Chemical polishing
Nb/Nb2O3, E-Ni-Fe - Chemical-Mechanical polishing
Nb2O5 - Chemical etching
Nb2O5 as the natural mineral iron niobate FeNb2O6 - Chemical etching
Nb3B3 specimens - Chemical etching - General microstructure
Nb3B3 specimens - Chemical etching - General microstructure
Nb3B3 specimens - Chemical etching - General microstructure
Nb3Ge single crystal compound - Physical etching
Nb3Ge thin films on (100) Ge substrates - Chemical etching
Nb3Se (100) hexagonal platelets - Chemical cleaning
Nb3Si - Electrolytic etching
Nb3Sn - Anodizing
Nb3Sn - Chemical etching
Nb3Sn amorphous thin films - Heat, removal
Nb3Sn as single crystals - Chemical polishing
Nb3Te4 single crystal - Chemical cleaning
NbAl(y) as alloy specimens - Chemnical etching
NbC and NbC2 - Electrolytic etching
NbC specimens - Chemical etching
NbC specimens - Chemical etching
NbC thin films - Chemical etching
NbC/NbC2 - Electrolytic etching - General microstructure
NbH as powder - Chemical etching
NbH deposited on silicon wafers - Chemical etching - General microstructure
NbN (100) thin films deposited on NaCl - Ionized gas cleaning
NbN (yellow), Nb2N (pink) - Electrolytic etching - General microstructure
Niobium (high purity) - Etch pit etching
Niobium - Attack polishing
Niobium - Cathodic etching
Niobium - Chemical etching
Niobium - Chemical etching
Niobium - Chemical etching
Niobium - Chemical etching
Niobium - Chemical polishing
Niobium - Chemical polishing
Niobium - Chemical polishing
Niobium - Chemical polishing
Niobium - Chemical polishing
Niobium - Chemical polishing
Niobium - Cr, Nb, and alloys - General microstructure
Niobium - Dislocation etching
Niobium - Dislocation etching
Niobium - Dislocation etching
Niobium - Dislocation etching
Niobium - Dislocation etching
Niobium - Dislocation etching
Niobium - EBSD sample preparation - Dislocation etching
Niobium - Electrolytic etching
Niobium - Electrolytic polishing
Niobium - Electrolytic polishing
Niobium - Electrolytic polishing
Niobium - Electrolytic polishing
Niobium - Electrolytic polishing
Niobium - Electrolytic polishing
Niobium - Electrolytic polishing
Niobium - Electrolytic polishing
Niobium - Electrolytic polishing
Niobium - Electrolytic polishing
Niobium - Electrolytic polishing
Niobium - Electrolytic thinning
Niobium - Electrolytic thinning
Niobium - Electrolytic thinning
Niobium - Electrolytic thinning
Niobium - Electrolytic thinning (wire)
Niobium - Electrolytic thinning by window technique
Niobium - Electrolytic thinning by window technique
Niobium - Electromechanical polishing
Niobium - Etch pits etching
Niobium - Final electrolytic polishing
Niobium - For dislocation etch pits
Niobium - Mo, Ta, Nb, Mo-Ti alloys, Ta-Nb alloys, Pure V and V base alloys
Niobium - Mo, W, V, Nb, Ta and their alloys
Niobium - Nb, Ta, Mo and their alloys
Niobium - Ta and Ta base alloys, Nb and Nb base alloys
Niobium - Ta base alloys, Nb base alloys
Niobium - Ta base and Nb base alloys
Niobium - Ta, Nb, and their alloys, Cr and Cr silicide, Re silicide, W-Th alloys
Niobium - Twin jet electrolytic polishing
Niobium carbide (NbC) - Dislocation etching
Niobium carbide (NbC) - Thermal etching
Niobium oxide (NbO, Nb2O3, Nb2O5) - Chemical etching - General microstructure
Niobium single crystal - Chemical polishing
Niobium single crystal - Electrolytic polishing
Niobium single crystal - Electrolytic polishing
Niobium single crystal - Produces triangular etch pits on (111) planes
Niobium specimens - Chemical etching - General microstructure
Niobium specimens - Chemical etching - General microstructure
Niobium specimens - Chemical etching - General microstructure
Niobium specimens - Chemical etching - General microstructure
Niobium specimens - Chemical etching - General microstructure
Niobium specimens - Chemical etching - General microstructure
Niobium-Tin (Nb-Sn) - Nb3Sn - General microstructure
Niobium-tin (Nb-Sn) - Chemical thinning
Oxide ceramics - Nb oxides, NbO (blue), NbO2 (cyan), Nb3O3 (red-dish-brown)
Pelleg's electrolytic polishing solution - Niobium - Dislocation etching
Picklesimer's anodizing solution - Nb and alloys - Electrolytic etching
Picklesimer's solution - Nb-Ti alloy - Anodising
Picklesimer's solution - Nb-Ti alloys
Pure Nb - Electrolytic etching