Etchants for Palladium and Alloys

ASTM etchant No. 165a - Pd alloys - Electrolytic etching
ASTM etchant No. 165a - Pure palladium - Electrolytic etching
ASTM etchant No. 166 - Pd alloys
ASTM etchant No. 166 - Pd alloys - Chemical etching
ASTM etchant No. 166 - Pure palladium - Chemical etching
ASTM etchant No. 61 - >90% noble metals - Chemical etching
ASTM etchant No. 61 - >90% noble metals - Chemical etching
ASTM etchant No. 61 - Pure palladium - Chemical etching
ASTM etchant No. 62 - Pd alloys - Chemical etching
ASTM etchant No. 62 - Pure palladium - Chemical etching
ASTM etchant No. 64a - Pd alloys - Chemical etching
ASTM etchant No. 65 - <90% noble metals - Chemical etching
Adler's etchant - Pd-Ga alloy (Pd5Ga2) - Chemical etching
Agua regia - Pd-H as powdered "Palladium Black" with absorbed hydrogen
Agua regia - PdAg alloy - Chemical etching
Agua regia - PdNiP, PtNiP, and PtCuP metallic glasses - Chemical etching
Agua regia, dilute - Pd thin films - Chemical cleaning
Aqua regia - Pd thin film - Chemical cleaning
Aqua regia - PdAu deposited as a 11 mixture on glass, quartz, and aapphire substrates - Chemical etching
Palladium - Au alloys with less thn 90% content of precious metals - General microstructure
Palladium - Cathodic etching
Palladium - Chemical etching
Palladium - Chemical etching - General microstructure
Palladium - Electrolytic polishing
Palladium - Electrolytic polishing
Palladium - For Au alloys with high content of precious metals - General microstructure
Palladium - Os base alloys, pure Pd and Pd alloys, Pt-Au alloys, Ir
Palladium - Pure Au and Au-rich alloys, Pd and Pd alloys
Palladium - Pure Au and Pd, Au-Pd, Pd alloys with more than 90% concentration of precious metals
Palladium - Pure Pt and Pd, Au alloys
Palladium alloy - Grain contrast
Palladium alloys - Chemical etching - General microstructure
Palladium and palladium alloys - Electrolytic etching
Palladium specimen - Au, Pt alloys and Pd alloys
Palladium welded to Nickel-Silver (Pd, Ni-Ag) - Electric contact material
Palladium-Copper (Pd-Cu) - Electric contact material
Palladium-Platinum-Gold-Silver-Copper-Zinc (Pd-Pt-Au-Ag-Cu-Zn) - Electric contact material
Palladium-Ruthenium (Pd-Ru) - Electric contact material
Palladium-Silver (Pd-Ag) - Electric contact material
Pd 99.95% pure single crystal specimens - Electrolytic polishing
Pd and alloys - Chemical etching
Pd and alloys - Chemical etching
Pd and alloys - Chemical etching
Pd and alloys - Electrolytic etching
Pd single crystals and thin films - Chemical etching
Pd-Ag-Cu alloy - 35 at.% Ag-25 at.% Cu
Pd-Ce alloy - Alloys with 0-50% Ce
Pd-Ce alloy - Approx. Ce3Pd4
Pd-Ce alloy - Pd rich alloys
Pd-Ce alloy - Pd3Ce
Pd-Er alloy - Electrolytic and chemical etching
Pd-Er alloy - Er3Pd4 - General microstructure
Pd-Eu alloy - Approx. PdEu - General microstructure
Pd-Ga alloy - Sample preparation with different etching techniques
Pd-Gd alloys (Approx. Gd3Pd4) - Chemical etching - General microstructure
Pd-Gd alloys - Chemical and Electrolytic etching - General microstructure
Pd-Ge system - Pd(x)Ge(1-x), 0.75 <= x =<0.85
Pd-Hf alloys (Approx. 55 at.% Pd) - Chemical etching - General microstructure
Pd-Ho alloys (Approx. Ho3Pd4) - Chemical etching - General microstructure
Pd-Ho alloys - Chemical and electrolytic etching - General microstructure
Pd-Ni alloys - Chemical etching - General microstructure
Pd-Sm alloys - Chemical and electrolytic etching - General microstructure
Pd-U alloys (Up to 25 at.% U) - Chemical etching - General microstructure
Pd-Y alloys - Chemical and electrolytic etching - General microstructure
Pd-Zn system (Pd-45 at.% Zn) - Phsical thinning
Pd-Zn-Ga alloy - PdZn-PdGa pseudo-binary alloys
PdSi and PdSi2 thin films grown on silicon substrates - Chemical etching - General microstructure
Pure Pd - Chemical etching
Vilella's etchant - Pd dental alloys, Pd alloys with Al, Os, In, Sn, Fe, and Cu - Chemical etching