Etchants for Titanium and Alloys

1.5Sn-0.15Fe-0.10Cr, and Hf alloys - Chemical etching - General macrostructure
5% Al and 2.5% Sn and Ti, 6% Al, and 3% Sn and Ti alloys - Chemical etching
7A1-4Mo alloys - Chemical etching - General macrostructure
ASTM etchant No. 11 - Ti alloys - Chemical etching
ASTM etchant No. 158 - Ti alloys - Chemical etching
ASTM etchant No. 170a - Ti alloys - Chemical etching
ASTM etchant No. 178 - Ti alloys - Chemical etching
ASTM etchant No. 18 - Pure titanium - Electrolytic etching
ASTM etchant No. 186 - Pure titanium
ASTM etchant No. 186 - Pure titanium - Chemical etching
ASTM etchant No. 186 - Ti alloys - Chemical etching
ASTM etchant No. 187 - Kroll's etchant - Ti alloys
ASTM etchant No. 187 - Ti alloys - Chemical etching
ASTM etchant No. 188 - Pure titanium
ASTM etchant No. 188 - Pure titanium - Chemical etching
ASTM etchant No. 188 - Ti alloys - Chemical etching
ASTM etchant No. 189 - Ti-5 Al-2.5 Sn
ASTM etchant No. 189 - Ti-5 Al-2.5 Sn alloys - Chemical etching
ASTM etchant No. 190 - Ti-6 Al-6V-2 Sn
ASTM etchant No. 190 - Ti-6 Al-6V-2 Sn alloys - Chemical etching
ASTM etchant No. 191 - Ti-Al-Zr
ASTM etchant No. 191 - Ti-Al-Zr alloys - Chemical etching
ASTM etchant No. 192 - Kroll's etchant - Ti alloys
ASTM etchant No. 192 - Ti alloys - Chemical etching
ASTM etchant No. 192 - Ti alloys - Chemical etching
ASTM etchant No. 192 - Ti-13V-11Cr3 Al (aged) alloys - Chemical etching
ASTM etchant No. 192 - Ti-8Mn alloys - Chemical etching
ASTM etchant No. 193 - Ti-Si
ASTM etchant No. 193 - Ti-Si alloys - Chemical etching
ASTM etchant No. 194 - Ti alloys
ASTM etchant No. 194 - Ti alloys - Chemical etching
ASTM etchant No. 1c - Ti alloys - Chemical etching
ASTM etchant No. 1c - Ti alloys - Chemical etching
ASTM etchant No. 3a - Ti alloys - Chemical etching
ASTM etchant No. 67 - Pure titanium - Chemical etching
ASTM etchant No. 67 - Ti alloys - Chemical etching
ASTM etchant No. 68 - Pure titanium - Electrolytic etching
ASTM etchant No. 68 - Ti alloys - Electrolytic etching
ASTM etchant No. 69 - Pure titanium - Electrolytic etching
ASTM etchant No. 69 - Ti alloys - Electrolytic etching
Agua regia - Ti0.3W0.7Si2 thin films - Chemical polishing
Agua regia - Ti3W7Si2 thin films on silicon wafers, (111), (110) and (100) - Chemical etching - General microstructure
Agua regia - TiO2 single crystal natural rutile crystals - Chemical cleaning
Agua regia - TiW (1% Ti) thin films - Chemical etching - General microstructure
Alloy Ti42Si38 - Twin jet polishing mehod
Alloy Ti52Al48 - Twin jet polishing mehod
Alloy Ti52Al48 - Twin jet polishing mehod
Alloy Ti52Al48V1 - Twin jet polishing mehod
Alloy Ti83Co12Al5 - Twin jet polishing mehod
Alpha Ti - Chemical etching - General microstructure
Alpha-beta alloys - General macrostructure
B etchant - For Ti
BHF etchant - TiN thin films - Chemical etching - General microstructure
BHF etchant - TiN thin films deposited on poly-Si epitaxy layers - Chemical etching - General microstructure
Beraha's tint etchant - Cast Ti alloys - Tint etching
Beta-III titanium alloy - Ti-11.5Mo-5-6Zr-4.5Sn
Beta-III titanium alloy - Ti-11.5Mo-6Zr-4.5Sn
Beta-III titanium alloy - Ti-11.5Mo-6Zr-4.5Sn
Beta-III titanium alloys - Chemical polishing
Blackburn and William's solution - Ti-Mo alloy - Alloy with 11.6% Mo
Blackburn and William's solution - Ti-Mo-Al-Sn-Zr alloy - Titanium 6246-6Al-2Sn-4Zr-6 Mo
Blackburn and Williams's solution - Ti-Mo alloys
Blackburn-William's electrolyte - Ti-Al-Nb alloy - Ti3Al-Nb
Ceramics, borides - TiB2 - General microstructure
Ceramics, borides - TiB2 - General microstructure
Ceramics, carbides - TiC - General microstructure
Ceramics, carbides - TiC, TaC - General microstructure
Cermets - TiC-Ni - General microstructure
Cermets - TiCN-Co, TiN-Fe, TiN-Mo, TiN-W
Electrolytic polishing of pure titanium - EBSD sample preparation
Ence and Margolin's etching solution (H-etch) - Ti alloys - Electrolytic etching
Etchant for titanium aluminide - Chemical etching - General microstructure
Extraction replica etchant for titanium alloys - Chemical etching
Finlay's A etchant (Remington's A etchant) - For Ti and Ti/Zr
Finlays B etchant - For Ti
For most Ti materials and Ti alloys, Ti-Mn and Ti-V-Cr-Al alloys - Chemical etching - General microstructure
Gamma-TiAl and alpha 2-Ti3Al - Chemical etching
H etchant - Ti alloys
Heat treated Ti alloys - Chemical etching
Hydrides in Ti, alpha-beta alloys - Chemical etching - General microstructure
I.M.I. 685 alloy - Ti-6Al-6Zr-0.5Mo-0.25Si
Iodide Ti - Electrolytic etching
Iodide Ti - General macrostructure
Iodide Ti alloy - Chemical etching - General macrostructure
Iodide titanium - Chemical polishing
Jodid (high-purity, iodide-process) Ti - Chemical etching - General macrostructure
Keller's etchant - Ti alloys - Chemical etching
Keller's etchant - Ti alloys - Chemical etching - General microstructure
Keller's etchant - Ti, Ti-Al alloys - Dislocation etching
Keller's etchant - Ti-6% Al-4% V alloy, Ti-5% Al-2.75% Cr-1.25% Fe alloy, Ti-2.55% Al-3.75% Mn alloy - General macrostructure
Keller's etchant - Ti-Al-Mn, Ti-Al-V, and Ti-Al-Cr-Fe alloys, flow lines - Chemical etching
Kroll's etchant - For most Ti materials, especially for Ti-Al-V-(Sn) alloys - Chemical etching
Kroll's etchant - Ti alloys - Chemical etching
Kroll's etchant - Ti and alloy - Ti-6Al-2Sn-1.5Zr-1Mo-0.35Bi-0.1Si
Kroll's etchant - Ti-Al-Mo alloy - 5.8-9.7% Al, 0.5-8.2% Mo
Kroll's etchant - Ti-Al-O alloy - Ti-6-10% Al-0.04-0.12% O
Kroll's etchant - Ti-Al-V alloy (6Al-4V) - Chemical etching - General microstructure
Kroll's etchant - Ti-Mo alloy - Ti-26Mo
Kroll's etchant - Ti-Mo-V-Al-Fe alloy - Ti-8Mn-8V-3Al-2Fe - General microstructure
Kroll's etchant - Ti-Mo-Zr-Sn alloy - Ti-11Mo-6.6Zr-4.6Sn
Kroll's etchant - Ti-Ni alloys - Chemical etching
Kroll's etchant - Ti-V-Cr-Zr-Mo-Al alloy - Ti-8V-6Cr-4Zr-4Mo-3Al
Kroll's etchant - Titanium - For many Ti raw materials, especially for Ti-Al-V alloys
Kroll's etchant - Titanium and titanium alloy
Kroll's etchant - Titanium and titanium alloys - General purpose etch - For most titanium alloys
Kroll's etchant 2 - For Ti/Al
Murakami's etchant, modified - Ti-V-Mo alloys - Chemical etching
Murkami's etchant - TiC specimens - Chemical cleaning
NiTi shape memory and superelastic alloys - Chemical etching - General microstructure
Pure Ti - Electrolytic etching
Pure Ti - Electrolytic etching - General microstructure
Pure Ti and Ti alloys - Physical etching - General microstructure
Pure Ti and Ti alloys, grain-boundary etchant - Chemical etching
Pure Ti and alloys - Electrolytic etching
Pure Ti and alloys - Electrolytic etching
Pure Ti and alloys - Electrolytic etching
Pure Ti, Ti-base alloys - Electrolytic etching - General microstructure
Pure Ti, Ti-base alloys, Ti-Al-Mo alloys - Chemical etching - General macrostructure
Pure Ti, alpha Ti, Ti-Al-V-Sn alloys, ferro titanium - Chemical etching - General microstructure
R etchant - For Ti/Al, Ti/Zr
R or A etchant - Ti-Zr alloys - Chemical etching
R-etchant - Ti-Al and Ti-Al-Zr alloys - Chemical etching
RIE etchant - TiW thin films - Ionized gas etching
Remington A etchant - Ti alloys - Chemical etching
Remington B etchant - Titanium - Chemical etching
Remington's A etchant (Finlay's A etchant) - For Ti alloys
Rutile single crystal (TiO2) - Chemical polishing
Sn-containing Ti alloys - Chemical etching - General microstructure
Ti alloys - Chemical etching
Ti alloys - Chemical etching
Ti alloys - Chemical etching
Ti alloys - Chemical etching
Ti alloys - Chemical etching
Ti alloys - Chemical etching - General macrostructure
Ti alloys - Electrolytic etching
Ti alloys - General macrostructure
Ti alloys - General macrostructure
Ti alloys - General macrostructure
Ti alloys - General macrostructure
Ti alloys and Ti-Pd alloys (up to 42% Pd) - Chemical etching
Ti alloys, Ti-7% Mn alloy - General macrostructure
Ti alloys, Ti-Al-Mn alloys, flow lines, banded structure - Chemical etching - General macrostructure
Ti alloys, etches segregation - Chemical ecthing
Ti alloys, idendification of alpha and beta Ti - Chemical etching - General macrostructure
Ti alloys, removal of Cu deposits on the surface - Chemical etching - General microstructure
Ti alloys, removal of Sn deposits on the surface - Chemical etching
Ti and Ti alloy - Modified window technique
Ti and Ti alloys (single crystals) - Dislocation etching
Ti and Ti alloys - Electrolytic polishing - Dislocation etching
Ti and Ti alloys - Electrolytic polishing - Dislocation etching
Ti and Ti alloys - Electrolytic polishing - Dislocation etching
Ti and Ti alloys - Electrolytic polishing - Dislocation etching
Ti and Ti alloys - Electrolytic polishing - Dislocation etching
Ti and Ti alloys - Electrolytic polishing - Dislocation etching
Ti and Ti alloys - Electrolytic polishing - Dislocation etching
Ti and Ti alloys - Electrolytic polishing - Dislocation etching
Ti and Ti alloys - Electrolytic polishing - Dislocation etching
Ti and Ti alloys - Electrolytic polishing - Dislocation etching
Ti and Ti alloys - Electrolytic polishing - Dislocation etching
Ti and Ti alloys - Electrolytic polishing and chemical etching
Ti and Ti-base alloys, segregations, color etchant - Electrolytic etching
Ti and alloy - Sample preparation procedure
Ti and alloys (Battelle) - Chemical etching
Ti and alloys - Chemical etching
Ti and alloys - Chemical etching
Ti and alloys - Chemical etching
Ti and alloys - Chemical etching
Ti and alloys - Electrolytic etching
Ti and alloys - Heat etching
Ti borides - Electrolytic etching
Ti evaporated as thin films - Chemical etching - General microstructure
Ti rod (electrode) - Chemical cleaning
Ti sheet and alloys - Chemical cleaning
Ti sheet and alloys - Chemical etching - General microstructure
Ti sheet and alloys - Chemical etching - General microstructure
Ti sheet and alloys - Chemical etching - General microstructure
Ti sheet and alloys - Chemical etching - General microstructure
Ti sheet and alloys - Chemical etching - General microstructure
Ti sheet specimens - Chemical etching - General microstructure
Ti specimens - Chemical etching - General microstructure
Ti specimens - Chemical etching - General microstructure
Ti specimens - Chemical etching - General microstructure
Ti specimens - Chemical etching - General microstructure
Ti specimens - Chemical etching - General microstructure
Ti specimens - Chemical polishing
Ti specimens - Chemical polishing/etching
Ti specimens - Chemical polishing/etching
Ti specimens - Electrolytic polishing
Ti specimens - Electrolytic polishing
Ti specimens - Electrolytic polishing
Ti specimens - Electrolytic polishing
Ti specimens - Electrolytic polishing
Ti specimens - Electrolytic polishing
Ti specimens - Salt polishing
Ti specimens - Thermal etching
Ti specimens and thin films - Chemical etching - General microstructure
Ti specimens and thin films - Chemical etching - General microstructure
Ti specimens and thin films - Chemical etching - General microstructure
Ti specimens used for electroplating - Electrolytic polishing
Ti thin film deposit - Chemical etching - General microstructure
Ti thin film deposit - Chemical etching - General microstructure
Ti thin film evaporation in vacuum systems - Chemical etching - General microstructure
Ti thin films - Chemical etching - General microstructure
Ti thin films - Chemical etching - General microstructure
Ti thin films - Electrolytic oxidation
Ti, 5% Al and 2.5% Sn alloy - Chemical etching
Ti-12.6% V specimen - Chemical thinning
Ti-3% Al alloy, Ti-13% V-11% Cr-3% Al alloy, Ti-6% Al-4% V alloy - General macrostructure
Ti-4% Al-4% Mn alloy - General macrostructure
Ti-4% Al-4% Mn alloy - General macrostructure
Ti-5% Al-2.5% Sn alloy - General macrostructure
Ti-6Al-4V alloy - Chemical etching
Ti-7% Al-4% Mo alloy - General macrostructure
Ti-Ag alloy - Alloys with 10-26 at.% Ag
Ti-Al alloy ( <25% Al) - Chemical etching - General microstructure
Ti-Al alloy (< 25% Al) - Precipitate etching
Ti-Al alloy (30% Al) - Electrolytic polishing
Ti-Al alloy (Ti-4Al) - Chemical polishing
Ti-Al alloy (Ti-8.6-10Al) - Electrolytic polishing
Ti-Al alloy - Alloy with 5% Al - General microstructure
Ti-Al alloys (3-46% Al) - Electrolytic polishing
Ti-Al alloys (5% Al) - Electrolytic thinning
Ti-Al alloys (Ti rich) - Electrolytic polishing and micro etching
Ti-Al alloys - Alloys with up to 40% Al
Ti-Al alloys - Chemical etching - General microstructure
Ti-Al alloys - Chemical etching - General microstructure
Ti-Al alloys - Chemical etching - General microstructure
Ti-Al alloys - Electrolytic thinning
Ti-Al alloys - Ti rich alloys - General microstructure
Ti-Al system - Alloys with up to 5 at.% Al - General microstructure
Ti-Al-B alloy - Alloy with 5% Ti and 1% B
Ti-Al-B alloys - Chemical etching - General microstructure
Ti-Al-Mn alloy - Electrolytic thinning
Ti-Al-Mn alloy - Electrolytic thinning in PTFE holder
Ti-Al-Mn alloys, flow lines - Chemical etching - General macrostructure
Ti-Al-Mo alloy - 8Al-1Mo-1V - General microstructure
Ti-Al-Mo alloy - Alloy with 6% Al and 2% Mo
Ti-Al-Mo-V alloy - 4-8% Al, 1-3% Mo, 1% V
Ti-Al-Mo-V alloy - 8Al-1Mo-1V - General microstructure
Ti-Al-Mo-V alloy - Chemical etching - General microstructure
Ti-Al-Mo-V alloy - Ti-811 (Ti-8Al-1Mo-1V)
Ti-Al-Mo-V alloy - Ti-8Al-1Mo-1V
Ti-Al-Nb-Ta alloy - Electrolytic thinning
Ti-Al-Nb-Ta-Mo alloy - Ti-6Al-2Nb-1Ta-0.8Mo - General microstructure
Ti-Al-Ni, Ti-Al-Sn, and Ti-Si alloys, hydrides - Chemical etching - General microstructure
Ti-Al-Si alloy (< 10% Al, 1% Si) - Chemical etching - General microstructure
Ti-Al-Sn alloy - Alloy with 2.5-5% Sn, 7-14.5% Al
Ti-Al-Sn alloy - Alloy with 5% Al and 2.5% Sn
Ti-Al-Sn alloy - Alloy with 5% Al and 2.5% Sn
Ti-Al-Sn alloy - Alloys with 5% Al and 2.5% Sn
Ti-Al-Sn alloy - Chemical etching - General microstructure
Ti-Al-Sn-Zr-Mo alloy - Ti-6Al-2Sn-4Zr-2Mo
Ti-Al-V alloy (5.9-9.7% Al, 2-6% V) - Chemical etching - General microstructure
Ti-Al-V alloy (6% Al, 4% V) - Chemical etching - General microstructure
Ti-Al-V alloy (6% Al, 4% V) - Electrolytic thinning
Ti-Al-V alloy (6Al-4V) - Chemical etching - General microstructure
Ti-Al-V alloy (6Al-4V) - Chemical etching - General microstructure
Ti-Al-V alloy (6Al-4V) - Chemical etching - General microstructure
Ti-Al-V alloy (6Al-4V) - Chemical polishing
Ti-Al-V alloy (6Al-4V) - Chemical polishing
Ti-Al-V alloy (6Al-4V) - Electrolytic polishing
Ti-Al-V alloy (6Al-4V) - Electrolytic thinning
Ti-Al-V alloy (6Al-4V) - General microstructure
Ti-Al-V alloy - Alloy with 6% Al and 4% V - General microstructure
Ti-Al-V alloy - Electrolytic thinning
Ti-Al-V alloys - Chemical etching - General microstructure
Ti-Al-V-Sn alloy - Alloy with 6% Al, 6% V and 2% Sn
Ti-Al-V-Sn alloy - Alloy with 6% Al, 6% V and 2% Sn
Ti-Al-V-Sn alloy - Ti-6Al-6V-2Sn alloy
Ti-Al-V-Sn alloy - Ti-6Al-6V-2Sn alloy
Ti-Al-Zr alloys - Alloys with 4.6-4.9% Al and 2-4% Zr
Ti-Al-Zr-Mo-Si alloy - Ti-6Al-6Zr-0.5Mo-0.25Si
Ti-Al-Zr-W-Si alloys - Electrolytic polishing and chemical etching
Ti-Au alloys - For alloys with 4 - 20 at.% Au - General microstructure
Ti-B system - Ti-TiB eutectic - General microstructure
Ti-Be alloys - For alloys with < 10% Be
Ti-Bi alloy (Ti-3.1 at.% Bi) - Chemical etching - General microstructure
Ti-C alloy - Potentiometric etching
Ti-C system - Ti-TiC section
Ti-C system - TiC(x), 0.5 < x < 1.0 - Single crystal
Ti-Co alloy - Alloy with 5% Co - General microstructure
Ti-Co alloy - F.c.c low Ti alloys - General microstructure
Ti-Co alloy - Ti - 3/8 at.% Co - General microstructure
Ti-Cr alloy - Ti - 10-20 at.% Cr - Electrolytic thinning
Ti-Cr alloy - Ti-6% Cr - General microstructure
Ti-Cr alloys - Chemical etching - General microstructure
Ti-Cr-V-Al alloy - 13% Cr, 11% V, 8% Al
Ti-Cr-V-Al alloy - 13Cr-11V-3Al - Electrolytic polishing
Ti-Cr-V-Al alloy - 13V-11Cr-3Al - Chemical polishing
Ti-Cu alloy - Electrolytic thinning by Mirand-Saulnier technique
Ti-Cu alloy - For alloys with 5% Cu
Ti-Cu alloys (approx. Ti2Cu) - Chemical etching - General microstructure
Ti-Cu alloys - Chemical etching
Ti-Cu alloys - Chemical etching - General microstructure
Ti-Cu alloys - Chemical etching - General microstructure
Ti-Fe alloy - Ti-4.5-13 at.% Fe
Ti-Mn alloy (10% Mn) - Electrolytic polishing
Ti-Mn alloy (8% Mn) - Electrolytic polishing and chemical etching
Ti-Mn alloy - Alpha-Beta alloys
Ti-Mn alloy - Ti-8.6 at.% Mn
Ti-Mn alloys - Chemical etching - General microstructure
Ti-Mo alloy (11% Mo) - Chemical etching - General microstructure
Ti-Mo alloy (11-17 at.% Mo) - Electrolytic thinning
Ti-Mo alloy (15% Mo) - Electrolytic polishing
Ti-Mo alloy (15.2 at.% Mo) - Chemical polishing
Ti-Mo alloy (7 at.% Mo) - Chemical etching - General microstructure
Ti-Mo alloy - Electrolytic thinning
Ti-Mo alloys (2-10% Mo) - Chemical etching - General microstructure
Ti-Mo-Zr-V-Al alloy - Electrolytic thinning
Ti-Nb diffusion couple - Electrolytic etching
Ti-Ni alloys (8-14 at.% Ti) - Jet electrolytic polishing
Ti-Ni alloys (Ni-12% Ti) - Electrolytic polishing
Ti-Ni alloys (Ti-3/5 at.% Ni) - Chemical etching - General microstructure
Ti-Ni-Cr alloy - TiNi-2/8% Cr - General microstructure
Ti-Ni-Si alloy - TiNi-1.3/5% Si
Ti-O-H alloy - Attack polishing
Ti-O-H alloys - Chemical etching - General microstructure
Ti-P alloys - General microstructure
Ti-Pb alloy (Ti-5.3 at.% Pb) - Chemical etching - General microstructure
Ti-Pd alloys (Ti rich) - Chemical etching - General microstructure
Ti-Pd alloys (Ti-8 at.% Pd) - Chemical etching - General microstructure
Ti-Si alloy - Ti-0.5/1.5 at.% Si
Ti-Si alloys - Chemical etching
Ti-Si system (Ti-Ti5Si3 eutectic) - Chemical etching - General microstructure
Ti-Sn alloys (10-40% Sn) - Electrolytic thinning
Ti-Sn alloys (up to 25% Sn) - Chemical etching
Ti-Ta alloy - Chemical etching and thinning
Ti-TiAg-Ag thin films - Chemical etching - General microstructure
Ti-V alloy (20% V) - Electrolytic thinning
Ti-V alloy - Electrolytic thinning
Ti-V alloy - Electrolytic thinning
Ti-V alloy - Electrolytic thinning and jet etching
Ti-V alloys (>20% V) - Dislocation etching
Ti-V alloys (15.5% V) - Chemical etching - General microstructure
Ti-V alloys (5-20% V) - Chemical etching and electrolytic thinning
Ti-V alloys (Beta alloys, 20-40 wt.% V) - Chemical polishing and elecytrolytic etching
Ti-V alloys - Chemical polishing
Ti-V-Cr-Al-Mo-Zr alloy - Beta C Ti-3Al-8V-6Cr-4Mo-4Zr
Ti-V-Cr-Al-Mo-Zr alloy - RMI (38-6-44) alloy Ti-3.5Al-8V-6Cr-4Mo-4Zr
Ti-V-Cr-Zr-Mo-Al alloy - Ti-3Al-8V-6Cr-4Zr-4Mo
Ti-V-Fe-Al alloy - Electrolytic polishing, chemical etching, electrolytic thinning
Ti-V-Si alloy - Ti-40V-1Si - Electrolytic polishing
Ti-Zr alloy (2% Ti) - Electrolytic thinning
Ti-Zr alloy (25 at.% Ti) - Chemical thinning and polishing
Ti2O3 specimens and thin films - Chemical etching - General microstructure
Ti3SiC2 (titanium silicon carbide) - Chemical etching - General microstructure
Ti6Al4V alloy - Chemical etching - General microstructure
TiB2 - Chemical etching
TiB2 - Chemical etching
TiB2 - Chemical etching
TiB2 - Chemical etching - General microstructure
TiB2 - Chemical etching - General microstructure
TiB2 - Chemical etching - General microstructure
TiB2 - Chemical etching - General microstructure
TiB2 - Electrolytic etching - General microstructure
TiB2 and TiC single crystal wafers - Cleaning
TiB2, ZrB2 - Chemical etching - General microstructure
TiC (001) cleaved wafers - Electrolytic etching - General microstructure
TiC (001) cleaved wafers - Polishing
TiC (100) thin films - Electrolytic polishing
TiC (100) wafers - Gas cleaning
TiC and TaC - Electrolytic etching
TiC coated steel - Structure of titanium carbide layer
TiC coated steel - This solution revealed a good grain boundry pattern in titanium carbide layer
TiC single crystal ingot - Electrolytic polishing
TiC-C alloys - Electrolytic etching
TiD2 as thin films - Chemical etching - General microstructure
TiN thin films deposited on (100) silicon wafers - Chemical etching - General microstructure
TiN thin films deposited on Ti (0001) substrates - Chemical etching - General microstructure
TiN thin films deposited on poly - Si-Ionized gas etching
TiN thin films deposited on poly-Si - Chemical etching - General microstructure
TiN thin films deposited on silicon wafers - Chemical etching - General microstructure
TiO2 (001) basal oriented wafers - Chemical cleaning
TiO2 (110) natural single crystal rutile specimens - Salt flux decoration
TiO2 - Chemical etching - General microstructure
TiO2 - Chemical polishing
TiO2 - Dislocation etching
TiO2 - Physical etching - General microstructure
TiO2 as a native oxide on titanium substrates - Chemical ecthing
TiO2 as natural minerals - Chemical etching - General microstructure
TiO2 as natural single crystal rutile - Chemical cleaning
TiO2 as natural single crystal rutile - Gas cleaning
TiO2 natural rutile specimens - Chemical cleaning
TiO2 thin film deposited on GaAs (100) substrates - Chemical etching - General microstructure
TiO2 thin film deposits - Chemical etching - General microstructure
TiO2 thin films deposited on (111), n-type silicon substrates - Chemical etching - General microstructure
TiO2 thin films deposited on GaAs (100) substrates - Ionized gas cleaning
TiSi thin films grown on (100) silicon wafers - Chemical etching - General microstructure
TiSi2 arc melted - Chemical polishing
TiSi2 thin film formed on silicon (100) substrates - Chemical etching - General microstructure
TiSi2 thin film grown on Si substrates - Chemical etching - General microstructure
TiSi2 thin films deposited on silicon wafers - Ionized gas etching
TiSi2 thin films grown on silicon substrates - Acid oxidation
TiW thin films - Chemical etching - General microstructure
Titanium - Attack polishing
Titanium - Attack polishing
Titanium - Attack polishing
Titanium - Attack polishing
Titanium - Attack polishing
Titanium - Attack polishing
Titanium - Cathodic etching
Titanium - Chemical etching
Titanium - Chemical etching - General microstructure
Titanium - Chemical etching - General microstructure
Titanium - Chemical etching - General microstructure
Titanium - Chemical etching - General microstructure
Titanium - Chemical etching - General microstructure
Titanium - Chemical polishing
Titanium - Chemical polishing
Titanium - Chemical polishing
Titanium - Chemical polishing
Titanium - Chemical polishing
Titanium - Chemical polishing
Titanium - Chemical thinning
Titanium - Differentiation of alpha and beta Ti
Titanium - Dislocation etching
Titanium - Electrolytic etching - General microstructure
Titanium - Electrolytic polishing
Titanium - Electrolytic polishing
Titanium - Electrolytic polishing
Titanium - Electrolytic polishing
Titanium - Electrolytic polishing
Titanium - Electrolytic polishing
Titanium - Electrolytic polishing
Titanium - Electrolytic polishing
Titanium - Electrolytic polishing
Titanium - Electrolytic polishing
Titanium - Electrolytic polishing
Titanium - Electrolytic polishing
Titanium - Electrolytic polishing
Titanium - Electrolytic polishing
Titanium - Electrolytic polishing
Titanium - Electrolytic polishing
Titanium - Electrolytic polishing
Titanium - Electrolytic polishing
Titanium - Electrolytic polishing
Titanium - Electrolytic polishing
Titanium - Electrolytic polishing
Titanium - Electrolytic polishing
Titanium - Electrolytic polishing
Titanium - Electrolytic polishing
Titanium - Electrolytic polishing
Titanium - Electrolytic polishing
Titanium - Electrolytic polishing
Titanium - Electrolytic polishing and chemical etching
Titanium - Electrolytic thinning
Titanium - Electrolytic thinning
Titanium - Electrolytic thinning by Mirand-Saulnier technique
Titanium - Electrolytic thinning by window technique
Titanium - Electrolytic thinning in RTFE holder
Titanium - Good general-purpose electrolyte
Titanium - Iodide Ti - General macrostructure
Titanium - Most types of Ti and Ti alloys, Ti-Mn, Ti-V-Cr-Al alloys
Titanium - One of the best electrolyte for universal use
Titanium - Physical etching - General microstructure
Titanium - Physical etching - General microstructure
Titanium - Pure Ti and Ti base alloys - General microstructure
Titanium - Sample preparation procedure
Titanium - Thermal etching
Titanium - Ti alloys - General microstructure
Titanium - Ti and Ti alloys, Grain boundary etchant
Titanium - Ti and Ti base alloys - Tint etching - Precipitates
Titanium - Ti and Ti base alloys, Ti-Al-Mo alloys
Titanium - Ti, Ferro Ti, Ti-Al-V-Sn alloys
Titanium - Ti-Al-Sn and Ti-Al-Ni alloys
Titanium - Welded seams - General macrostructure
Titanium - Zr, Ti, U, steels, superalloys
Titanium 500 alloy - Chemical etching - General microstructure
Titanium 600 alloy - Chemical etching - General microstructure
Titanium alloys - Color etching - Alpha titanium grains
Titanium alloys - Color etching - General microstructure
Titanium alloys - Color etching - General microstructure
Titanium alloys - Electrolytic polishing
Titanium alloys - Electrolytic polishing
Titanium alloys - Thermal etching - General microstructure
Titanium alloys, welds - Chemical etching - General macrostructure
Titanium alpha-Ti single crystal - Chemical polishing
Titanium and its alloys - Al-4Mo alloys
Titanium and its alloys - Chemical etching - General macrostructure
Titanium and its alloys - Ti alloys, De-smut Ti, -13 V, -11Cr, -3Al alloys
Titanium and titanium alloys - Chemical etching - General microstructure
Titanium and titanium alloys - Chemical etching - General microstructure
Titanium and titanium alloys - Chemical etching - General microstructure
Titanium and titanium alloys - Chemical polish and etch - For most titanium alloys
Titanium and titanium alloys - Electrolytic polishing
Titanium and titanium alloys - Electrolytic polishing
Titanium and titanium alloys - For Ti-Si alloys
Titanium and titanium alloys - General purpose etch
Titanium and titanium alloys - General purpose etch - For Ti-3Al-8V-6Cr-4Mo-4Zr alloy
Titanium and titanium alloys - General purpose etch - For Ti-8Mn; aged Ti-13V-11Cr-3Al
Titanium and titanium alloys - General purpose etch - For Ti-Al-Zr and Ti-Si alloys
Titanium and titanium alloys - General purpose etch - For most titanium alloys
Titanium and titanium alloys - Nonstaining etch - For most titanium alloys
Titanium and titanium alloys - Removes stain - For most titanium alloys
Titanium and titanium alloys - Reveals alpha case - For most titanium alloys
Titanium and titanium alloys - Reveals hydrides - For unalloyed titanium
Titanium and titanium alloys - Reveals hydrides - For unalloyed titanium
Titanium and titanium alloys - Stains alpha, transformed beta - For alpha-beta Titanium alloys
Titanium boride (TiB2) - For revealing structure of TiB2
Titanium boride TiB2 - Chemical etching - General microstructure
Titanium carbide (TiC) - Chemical and electrolytic etching - General microstructure
Titanium carbide (TiC) - Electrolytic polishing and chemical etching
Titanium carbide (TiC) - Electrolytic thinning
Titanium carbide (TiC) - TiC(0.97)
Titanium carbide (TiC) single crystal - Electrolytic polishing
Titanium diboride (B-Ti(2)) - Chemical etching - General microstructure
Titanium diboride (B-Ti(2)) - Chemical etching - General microstructure
Titanium diboride (B-Ti(2)) - General microstructure
Titanium diboride single crystals (B-Ti(2)) - Chemical etching - General microstructure
Titanium dioxide (TiO2) - Chemical etching - General microstructure
Titanium nitride (TiN)-Molybdenum cermets (MoO3) - Chemical etching
Titanium oxide (Rutile-TiO2) - Chemical etching - General microstructure
Titanium silicide (TiSi2) - Chemical etching - General microstructure
Titanium-gallium alloys (Ti-Ti3Ga) - Chemical etching - General microstructure
Weck's color etchant - Etchant/procedure to examine for overheated titanium - Chemical etching
Weck's etchant - Pure Ti and Ti alloys
Weck's etchant - Pure Ti and Ti alloys - Chemical etching
Weck's tint etch for alpha Ti - Chemical etching - General microstructure
Weck's tint etch for alpha Ti alloys - Chemical etching - General microstructure
Weck's tint etchant - Ti and alloys - Tint etching
Weck's tint etchant - Ti and alloys - Tint etching
Wiliams-Blackburn's etchant - Ti-Mo-Al-Cr alloy - Ti-4.5Al-5Mo-1.5Cr
Williams's solution - For Ti and alloys - Electrolytic polishing

Copyright © 2017 by Steel Data. All Rights Reserved.