Etchants for Uranium and Alloys

(U,Pu)C - Chemical etching - General microstructure
ASTM etchant No. 170a - U Beryllides - Chemical etching
ASTM etchant No. 195 - Pure uranium
ASTM etchant No. 195 - Pure uranium - Electrolytic etching
ASTM etchant No. 195 - U alloys - Electrolytic etching
ASTM etchant No. 196 - Pure uranium
ASTM etchant No. 196 - Pure uranium - Chemical etching
ASTM etchant No. 196 - U alloys - Chemical etching
ASTM etchant No. 207 - U alloys
ASTM etchant No. 207 - U alloys - Chemical etching
ASTM etchant No. 209 - W-Th alloys - Chemical etching
ASTM etchant No. 67 - Pure uranium - Chemical etching
ASTM etchant No. 67 - U alloys - Chemical etching
ASTM etchant No. 68 - U + Zr alloys - Electrolytic etching
ASTM etchant No. 69 - Pure uranium - Electrolytic etching
ASTM etchant No. 69 - U alloys - Electrolytic etching
Accary etchant - U-C alloys - Electrolytic etching
Accary etchant - Uranium - Chemical etching
Accary etchant - Uranium - For etching U carbide
Alpha-U specimens - Electrolytic polishing
Alpha-U specimens - Electrolyticlytic cleaning
Ambler and Slattery's etchant - UO2 - Chemical etching
Ambler and Slattery's etchant - Uranium - Electrolytic etching
Bright-field etchant for U - Electrolytic etching
Ceramics, carbides - (U, Pu)C high in U. UC-PuN mixtures
Ceramics, carbides - (U, Ou)C high in Pu - General microstructure
Ceramics, carbides - (U, Pu)C - General microstructure
Ceramics, carbides - UC, U(C, O), UC-UC2, UC2-U2C3 mixtures, (U, Pu)C high in C, U(C, N) UC-ZrC
Ceramics, carbides - UC-Cr23C6 mixtures
Ceramics, carbides - UC-Pu mixtures - General microstructure
Ceramics, nitrides - UN - General microstructure
Ceramics, nitrides - UN - General microstructure
Ceramics, nitrides - UN - General microstructure
Ceramics, nitrides - UN - General microstructure
Ceramics, nitrides - UN, UN-U2N mixtures - General microstructure
Ceramics, nitrides - UN-U(N2O)-U2N3 mixtures - General microstructure
Ceramics, nitrides - UN-U2N3 mixtures - General microstructure
Cermets - PuC-Pu - General microstructure
Cermets - UN-U, UN-W - General microstructure
Cermets - UO2-Al - General microstructure
Cermets - UO2-Cr - General microstructure
Cermets - UO2-Mo - General microstructure
Cermets - UO2-Nb - General microstructure
Cermets - US-Co, UC22-Fe, (UZr)C-Nb, (UZr)C-Ta, (UZr)C-W
Color etch for U3Si - Chemical etching
Gamma phases in U-Mo alloys - Electrolytic etching
High-purity U - Electrolytic etching
Kalling's etchant - UCe2 specimen - Chemical polishing
Kalling's etchant - UCo2 specimen - Chemical polishing
Kalling's etchant - UNi2 specimen - Chemical polishing
Kalling's etchant - UPt3 specimen - Chemical polishing
Murakami's etchant - U-Zr alloys - Chemical etching
Murakami's etchant - U-Zr alloys, U-Fe-Co alloys, U-Al2-U3Si3 alloys - Chemical etching
Oxide ceramics (U, Th, Pu)-UO2, ThxUyO2 (toxic), PuO2, cast (toxic), PuO2 (gamma, sintered)-toxic
Oxide ceramics - U4O9 (toxic) - General microstructure
Oxide ceramics - UO2 - General microstructure
Oxide ceramics - UO2 - General microstructure
Oxide ceramics - UO2 - General microstructure
Oxide ceramics - UO2 - Grain size
Oxide ceramics - UO2, UO2-PuP2, UO2-U4O9 and UO2-CeO2 mixtures
Oxide ceramics - UO2-PuO2 mixtures - General microstructure
Phosphides, sulfides - UO - General microstructure
Phosphides, sulfides - US - General microstructure
Picklesimer's anodizing solution - U alloys - Electrolytic etching
Pure U and U alloys - Chemical etching - General macrostructure
Pure U and U alloys - Chemical etching - General microstructure
Pure U and most U alloys - Electrolytic etching - General macrostructure
Pure U, pure Th - Electrolytic etching - General microstructure
U alloy and 2% Zr - Electrolytic etching
U alloys (U-N-Mo alloys) - Physical etching - General microstructure
U alloys - Chemical etching
U alloys - Chemical etching - General microstructure
U alloys - Electrolytic etching
U alloys and 10% Nb alloys - Chemical etching
U alloys and 5% fission products - Electrolytic etching
U and 5% fission products - Chemical etching
U and U alloy - Anodising etching solution
U and U alloys - Electrolytic etching - General microstructure
U and U alloys - Electrolytic polishing - Dislocation etching
U and U alloys - Electrolytic polishing - Dislocation etching
U and U alloys - Electrolytic polishing - Dislocation etching
U and U alloys - Electrolytic polishing - Dislocation etching
U and U alloys - Electrolytic polishing - Dislocation etching
U and U alloys - Electrolytic polishing - Dislocation etching
U and U alloys - Electrolytic polishing - Dislocation etching
U and U alloys - Electrolytic polishing - Dislocation etching
U and U alloys - Electrolytic polishing - Dislocation etching
U and U alloys - Electrolytic polishing - Dislocation etching
U and U alloys - Electrolytic polishing - Dislocation etching
U and alloys - Chemical etching
U and alloys - Electrolytic etching
U and alloys - Electrolytic etching
U and alloys - Electrolytic etching
U beryllides and U-Zr and U-Nb alloys - Chemical etching
U carbide - Chemical etching
U silicides, U-Zr, U-Ti, U-Zr-Mo alloys - Chemical etching
U specimens - Chemical cleaning
U specimens - Chemical cleaning
U specimens - Chemical polishing
U specimens - Chemical polishing
U specimens - Chemical polishing
U specimens - Electrolytic polishing
U specimens - Electrolytic polishing
U(C, N) specimens - Ceramic compunds - General microstructure
U(C, O) specimens - Ceramic compunds - General microstructure
U, Pu - Chemical etching - General microstructure
U, Pu, Am - Chemical etching - General microstructure
U-10Nb alloys - Chemical etching - General microstructure
U-2% Zr alloy - Sample preparation procedure
U-Al alloys - Chemical etching
U-Al alloys - Chemical etching - General microstructure
U-Al alloys - Chemical etching and electrolytic etching
U-Al alloys - For alloys with very low uranium content
U-Al-Ni system - UAl2-NiAl section - General microstructure
U-Be alloys, U-Zr and U-Nb alloys - Chemical etching - General microstructure
U-C alloys - Electrolytic etching
U-C alloys - Electrolytic etching - General microstructure
U-Co alloys - Physical etching - General microstructure
U-Co-Al alloy - UCo2-UAl3 section
U-Cu system - Electrolytic polishing
U-Fe alloys - Chemical and electrolytic etching
U-Fe-C alloys - Electrolytic polishing
U-Mn system - Electrolytic polishing
U-Mo alloy (16 wt.% Mo) - Electrolytic etching - General microstructure
U-Mo alloy (5 at.% Mo) - Sample preparation
U-Mo alloy - Electrolytic thinning by Mirand-Saulnier technique
U-Mo alloys - Electrolytic etching and polishing
U-Mo alloys - Physical etching - General microstructure
U-Mo and U-Zr alloys - Chemical etching
U-Mo and U-Zr alloys with stabilized gamma phase - Chemical etching - General microstructure
U-Mo-Ti alloys - Attack polishing
U-N-P alloy - UN-UP pseudobinary
U-Nb alloy - Cathodic etching
U-Nb alloy - Sample preparation
U-Nb alloys - Potentiostatic etching
U-Nb-H alloys - Chemical etching - General microstructure
U-Nb-Mo alloy - Cathodic etching
U-Nb-Zr alloy - Alloy with 7.5 Nb-2.5Zr
U-Ni-Zr alloy (7.5% U, 2.5% Zr) - Electrolytic polishing and etching
U-Pd alloys (Approx. 55 at.% Pd) - Chemical etching - General microstructure
U-Pu alloys - Electrolytic polishing
U-Re alloys - Chemical and Electrolytic etching - General microstructure
U-Si alloy - Cathodic etching
U-Si alloys - Electrolytic etching
U-Ti alloys - Chemical etching
U-Zr alloy - Electrolytic polishing
U-Zr alloys (Zr rich) - Electrolytic polishing
U-Zr alloys - Chemical etching - General microstructure
U-Zr alloys - Electrolytic etching
U-Zr alloys - Electrolytic polishing
U2C3+UC2 specimens - Ceramic compunds - General microstructure
U3N4 specimens - Chemical etching - General microstructure
U3Si alloys - Chemical etching - General microstructure
U4O9 - Chemical etching - General microstructure
UB4, UB2 and UB12 specimens - Chemical etching - General microstructure
UB4, UB2, and UB specimens - Chemical etching - General microstructure
UC (001) wafers - Electrolyticlytic jet thinning
UC - Dislocation etching
UC single crystal wafers - Chemical etching - General microstructure
UC specimens - Chemical etching - General microstructure
UC+PuN specimens - Ceramic compunds - General microstructure
UC+PuN specimens - Ceramic compunds - General microstructure
UC+ZrC - Ceramic compunds - General microstructure
UC+ZrC - Ceramic compunds - General microstructure
UC, U(C,O) x U(C,N), UC-ZrC mixtures, UC-UC2, UC2-U2C3 mixtures,(U,Pu)C C-rich
UC2+UC - Ceramic compunds - General microstructure
UN (001) wafers - Electrolyticlytic jet thinning
UN+U(N, O)+U2N3 - Ceramic compunds - General microstructure
UN+U2N3 - Ceramic compunds - General microstructure
UN-PuN, UO2-PuO2 and irradiated UO2-PuO2 alloys - Chemical etching
UO2 + ZrO2 - Chemical etching - General microstructure
UO2 - Chemical etching
UO2 - Dislocation etching
UO2 - Electrolytic etching - General microstructure
UO2 - Thermal etching
UO2 and UO2CeO2 - Chemical etching
UO2 specimens - Chemical etching - General microstructure
UO2 specimens - Chemical etching - General microstructure
UO2 specimens - Electrolytic polishing
UO2 x Th(x)U(y)O2, PuO2 cast, PuO2 (gamma, sintered) - Chemical ecthing
UO2, U3Si - Attack polishing
UO2, UO2-CeO2, UO2-U4O9, and UO2-PuO2 mixtures - Chemical ecthing
UO2, UO2CeO2 - Attack polishing
UO2, carbide-coated graphite, pyrolitic graphite - Attack polishing
UO2-PuO2 mixtures - Chemical ecthing
UP - Chemical etching - General microstructure
US (001) wafers - Electrolyticlytic jet thinning
US - Chemical etching - General microstructure
US specimens - Chemical etching - General microstructure
UTi single crystal specimens - Electrolytic polishing
Uranium - Attack polishing
Uranium - Attack polishing
Uranium - Attack polishing
Uranium - Cathodic etching
Uranium - Cathodic etching
Uranium - Cathodic etching
Uranium - Chemical etching
Uranium - Chemical etching
Uranium - Chemical thinning and electrolytic polishing
Uranium - Electrolytic etching
Uranium - Electrolytic etching
Uranium - Electrolytic etching - General microstructure
Uranium - Electrolytic polishing
Uranium - Electrolytic polishing
Uranium - Electrolytic polishing
Uranium - Electrolytic polishing
Uranium - Electrolytic polishing
Uranium - Electrolytic polishing
Uranium - Electrolytic polishing
Uranium - Electrolytic polishing
Uranium - Electrolytic polishing
Uranium - Electrolytic polishing
Uranium - Electrolytic polishing
Uranium - Electrolytic polishing
Uranium - Electrolytic polishing
Uranium - Electrolytic polishing
Uranium - Electrolytic polishing
Uranium - Electrolytic polishing
Uranium - Electrolytic polishing and etching
Uranium - Electrolytic thinning
Uranium - Electrolytic thinning
Uranium - Electrolytic thinning
Uranium - Electrolytic thinning
Uranium - Electrolytic thinning
Uranium - Electrolytic thinning by Bollmann technique
Uranium - Electrolytic thinning by Mirand-Saulnier technique
Uranium - Electrolytic thinning in PTFE holder
Uranium - Gamma phase stablized U-Mo and U-Zr alloys
Uranium - Good general-purpose electrolyte
Uranium - One of the best electrolyte for universal use
Uranium - Pure U and Th - General microstructure
Uranium - U alloys - General microstructure
Uranium - U and U alloys - General macrostructure
Uranium - U and most U alloys - General macrostructure
Uranium - U and most U alloys - General microstructure
Uranium - U silicides - General microstructure
Uranium - U-Al alloys - General microstructure
Uranium - U-Be alloys, U-beryllides, U-Zr, and U-Nb alloys
Uranium - Zr, Ti, U, steels, superalloys
Uranium alloys - Color etching - Electrolytic etching
Uranium alloys - Color etching - Physical etching
Uranium alloys - Electrolytic polishing
Uranium and uranium alloys - Electrolytic etching
Uranium carbide (UC) - Chemical etching - General microstructure
Uranium carbide (UC) - Electrolytic polishing
Uranium carbide (UC) - Electrolytic polishing and etching
Uranium carbide (UC) - Electrolytic thinning
Uranium carbide (UC) - Physical etching - General microstructure
Uranium carbide (UC)-zirconium carbide (ZrC) system - Chemical etching - General microstructure
Uranium carbide (UC)-zirconium carbide (ZrC) system - Chemical etching - General microstructure
Uranium carbide-Lanthanum alloys
Uranium carbide-neodymium alloys (C-Nd-U)
Uranium carbides (UC, U2C3, UC2) - Chemical etching - General microstructure
Uranium dioxide (UO2) - A suitable etching method for determining grain size
Uranium dioxide (UO2) - Cathodic etching
Uranium dioxide (UO2) - Chemical etching - General microstructure
Uranium dioxide (UO2) - Chemical etching - General microstructure
Uranium dioxide (UO2) - Chemical etching - General microstructure
Uranium dioxide (UO2) - Chemical etching - General microstructure
Uranium dioxide (UO2) - Chemical etching - General microstructure
Uranium dioxide (UO2) - Chemical etching - General microstructure
Uranium dioxide (UO2) - Chemical thinning
Uranium dioxide (UO2) - Electrolytic thinning
Uranium dioxide (UO2) and higher oxides - Chemical etching - General microstructure
Uranium dioxide (UO2) single crystals - Used mainly for (111) faces but can be used for (100) faces
Uranium dioxide (UO2, irradiated) - Chemical etching - General microstructure
Uranium dioxide (UO2, irradiated) - Chemical etching - General microstructure
Uranium dioxide (UO2, irradiated) - Chemical etching - General microstructure
Uranium dioxide-carbon-nitrogen system - Chemical etching - General microstructure
Uranium dioxide-thoria system (10% UO4) - Chemical etching - General microstructure
Uranium nitride (UN) - Chemical etching
Uranium nitride (UN) - Chemical etching - General microstructure
Uranium nitride (UN) - Electrolytic polishing
Uranium oxide (U3O8) - Chemical etching - General microstructure
Uranium oxide (U4O9) - Chemical etching - General microstructure
Uranium oxide (UO2) - Chemical etching - General microstructure
Uranium oxide (UO2) - Chemical etching - General microstructure
Uranium oxide (UO2) - Electrolytic etching - General microstructure
Uranium oxide (UO2) - Electrolytic polishing
Uranium oxide (UO2) - Physical etching - General microstructure
Uranium oxide (UO2) - Physical etching - General microstructure
Uranium oxide (UO2) - Physical etching - General microstructure
Uranium phosphide - Chemical etching - General microstructure
Uranium phosphide - Chemical etching - General microstructure
Uranium silicon alloys - Chemical etching - General microstructure
Uranium silicon alloys - Distinguishes U3Si2, U3Si, alpha U and UC
Uranium silicon alloys - Distinguishes U3Si2, U3Si, alpha U and UC
Uranium silicon alloys - For U2Si2, U3Si, alpha U and UC
Uranium sulphide (US) - Chemical etching - General microstructure
Uranium-gallium alloys (U-Ga) - Chemical etching - General microstructure
Uranium-molybdenum alloys - Chemical etching - General microstructure
Uranium-osmium alloys (U-Os) - Chemical and electrolytic etching