Etchants for Y and Alloys

a-Ge evaporated on fused quartz blanks
a-SiC-H thin films deposited on Si (100) substrates-Chemical etching
Mg-Y alloy-Alloy with 10.8 wt.% Y
Mg-Y alloy-Alloy with 8.7% Y
Mn-Zn ferrite-low Y oxide body (Fe-Mn-O-Y-Zn)-Mn0.51 x Zn0.43 x Fe2.03 x O4 + Y2O3
Oxide ceramics-MgO, ThO2 (toxic), Al2NiO4, PuO3 (gamma, sintered)-toxic, Y2O3-ZrO2 and Sm2O3-ZrO2 mixtures
Pd-Y alloys-Chemical and electrolytic etching
Rare earths (Ce, Dy, Er, Eu, Gd, Ho, La, Lu, Nd, Pr, Sm, Sc, Tb, Tm, Yb, Y)-Sample preparation procedure
Thorium oxide (ThO2)-yttrium oxide (Y2O3)-10 mol.% ThO2-Chemical etching
Thorium oxide (ThO2)-yttrium oxide (Y2O3)-Chemical etching
Y single crystal specimens-Chemical etching
Y specimens-Chemical etching
Y specimens-Chemical etching
Y2O3 x ThO2
Y2O3 x ThO2
Y2O5
Y2O5
Y3Fe5O12 and Y3Fe4AlO12
Y3Fe5O12 and Y3Fe4AlO12
Y3Fe5O12
Y3Fe5O12
Y-Ag alloys-Chemical etching
Y-Al alloys-Electro polishing
Y-Al-C alloys
Y-Al-C alloys
Y-Bi system-Chemical etching
Y-C system-Electrolytic polishing
Y-Cd system-Chemical etching
Y-Cd-Zn alloys-Chemcial etching
Y-Gd-Tm-Ga-Fe garnet-Chemical etching for etch pits
Y-Ge system-Chemical ecthing
Y-Hf alloy-Chemical etching
Y-Mn alloys-Chemical etching
Y-N system-Up to 5 at.% N
Y-O system (up to 15. at.% O2)-Chemical ecthing
Y-Pb system-Chemical etching
Y-Pd alloys (approx. Y3Pd4)-Chemical etching
Y-Sb alloys-Pysical etching
Y-Ta alloys-Chemical etching
Y-Ta alloys-Chemical etching
Y-Ta alloys-Chemical etching
Y-Ti alloy-Chemical etching
Y-Ti, Y-Zr and Y-Hf alloys - M-etch
Y-Ti, Y-Zr and Y-Hf alloys - M-etch
Yttrium iron garnet (Y3Fe5O12)-Chemical ecthing
Yttrium iron garnet (Y3Fe5O12)-Chemical etching
Yttrium oxide (Y2O3)-Chemical etching
Yttrium oxide (Y2O3)-Dislocation etching
Yttrium silicate (Y5Si3Ox)-Chemical etching
Yttrium-aluminium garnets (Nd doped)-Chemical polishing
Yttrium-aluminium garnets-Chemical etching
Yttrium-aluminium garnets-Chemical polishing
Yttrium-Electrolytic polishing
Yttrium-Electrolytic polishing
Yttrium-niobium (Y-Nb) alloys-Chemical etching
Yttrium-niobium (Y-Nb) alloys-Chemical etching
Yttrium-niobium (Y-Nb) alloys-Nb rich alloys
Yttrium-ortoaluminate (YAlO2)-Chemical etching
Yttrium-Y
Yttrium-Y
Y-V alloys-Chemical etching
Y-V alloys-Chemical etching
Y-Zr alloy-Chemical etching
Zirconium-yttrium-oxygen system (Zr-Y2O3)-Chemical polishing