En 34 Steel

Material designation: En 34
Diagram No.: 1335
B.S. designation: En 34
Chemical composition in weight %: 0.16% C, 0.18% Si, 0.53% Mn, 0.011% S, 0.022% P, 1.56% Ni,
0.26% Cr, 0.25% Mo
Steel group: Ni-Mo case hardening steels
Applications: No data
Comment: McQuaid Ehn grain size: 5 (ASTM), as quenched grain size: 8 (ASTM)
Source: Not shown in this demo version.

Heat Treatment
End quench temperature: 865oC

Hardenability Diagram
Price: 40.00 US $