1.5864 Steel

Steel name: 1.5864
Steel names of producers:
W3-2536 BOFORS Sweden
NiCr18 Dirostahl Germany
NiCr18 Hover&Sohn Germany
NiCr18 Saarstahl Germany
TEW35NiCr18 Thyssen Edelstahl Service GmbH Germany
NiCr18 SEL Germany
KR75 BOFORS Sweden
NiCr18 Krupp Germany
Diagram No.: 4525
Type of diagram: CCT
Mat. No. (Wr. Nr.) designation: 1.5864
Chemical composition in weight %: 0.40% C, 0.25% Si, 0.25% Mn, 0.011% P, 0.009% S, 1.58% Cr, 4.35% Ni.
Note: Alloy special structural steels. Austenitizing temperature: 850oC.
Reference: Not shown in this demonstration version.

Transformation Diagram