0.05C-0.90Mn-1.20Si-0.40Mo Steel

Steel name: 0.05C-0.90Mn-1.20Si-0.40Mo
Diagram No.: 1945
Type of diagram: CCT
Chemical composition in weight %: 0.05% C, 0.90% Mn, 1.20% Si, 0.40% Mo, 0.00% Cr
Steel group: Chromium steels
Note: Austenitizing temperature: 1010oC (1850oF). Grain size: 5-6.
Diagram Description: PF-Polygonal ferrite, P-pearlite, CRmin CRmax-min and max cooling rates for obtaining good dual-phase structure in coiled strip, PFsPF75Ps-min times for PF-start, 75% PF, and P-start. See the diagrams No. 1946, No. 1947 and No. 1948.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.