Alphabetical Index
Chemical Composition
Keyword Search
AFNOR Steels
AISI/SAE Steels
BS Steels
DIN Steels
Wr.Nr. (Mat.No.) Steels
Calculated Diagrams
CCT Diagrams
TTE Diagrams
TTT Diagrams
TTP Diagrams
TTS Diagrams
Alloy Steels
Carbon Steels
Carburizing Steels
Cast Irons
Chromium Steels
Cold Work Tool Steels
High Speed Steels
Hot Work Tool Steels
Low Carbon Steels
Microalloyed Steels
Molybdenum Steels
New Diagrams
Nitriding Steels
Plastic Mould Steels
PM Steels
Stainless Steels
Steel Companies
Structural Steels
Tools Steels
Vanadium Steels
Welding Steels
White Cast Irons
Help
Home
0.37% C-0.8% Mn-0.3% Si-0.7% Cr-0.26% Mo Steel
Steel name: 0.37% C-0.8% Mn-0.3% Si-0.7% Cr-0.26% Mo
Diagram No.: 2036
Type of diagram: CCT
Chemical composition in weight %: 0.37% C, 0.85% Mn, 0.39% Si, 0.73% Cr, 0.26% Mo
Steel group: Molybdenum steels
Note: Austenitizing temperature: Ac3 + 30oC (54oF) for 20 min.
Reference: Not shown in this demo version.
Transformation Diagram
Price: 30.00 US $
Buy Online Transformation Diagram
Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.