0.38% C-V Steel

Steel name: 0.38% C-V
Diagram No.: 2216
Type of diagram: CCT
Chemical composition in weight %: 0.38% C, 1.63% Mn, 0.30% Si, 0.016% S, 0.018% P, 0.02% Cr, 0.01% Ni, 0.12% Mo, 0.07% V, 0.01% Cu, sol. 0.021% Al
Steel group: Quenched and tempered engineering steels, vanadium steels
Note: Austenitizing temperature: 920oC
Reference: Sumitomo Metal Industries Ltd, Central Research Laboratories, as published in Atlas of Continuous Cooling Transformation Diagrams for Vanadium Steels, Vanitec, England, June 1985.

Transformation Diagram


Click the image to enlarge the diagram.

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.