0.1% C - 13.0% Cr Steel

Steel name: 0.1% C - 13.0% Cr Steel
Diagram No.: 2535
Type of diagram: TTT
Chemical composition in weight %: 0.10% C, 0.48% Mn, 0.55% Si, 0.024% P, 0.011% S, 0.51% Ni, 13.30% Cr, 8.00% Co
Steel group: Stainless steels
Note: Austenitizing temperature: 1000oC (1830oF) for 1h. See the diagrams No. 2534 and No. 2536.
Reference: P. Nicolaides, et al., "Influence of Cobalt on the Transformation of a Chromium Alloyed Austenite", Transactions of the Metallurgical Society of AIME, Vol.215, August 1959, pp. 702-705.

Transformation Diagram


Click the image to enlarge the diagram.

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.