0.44 C Steel

Steel name: 0.44 C Steel
Diagram No.: 2763
Type of diagram: TTT
Chemical composition in weight %: 0.40% C, 0.24% Mo
Steel group: Structural steels
Note: Influence of applied pressure on transfomation. Steel at one atmosphere and ar 24 kbar, and comparison with TTT curve of 0.40% C steel at 24 kbar. See the diagrams No. 2761 and No. 2762.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.


















Copyright © 2019 by Steel Data. All Rights Reserved.