Carbon Steel

Steel name: Carbon Steel
Diagram No.: 2784
Type of diagram: TTP
Chemical composition in weight %: a.) 0.20% C, 0.023% Nb, 1.04% V, 15 ppm N, 13 ppm O. b.) 0.15% C, 0.020% Nb, 0.75% V, 40 ppm N, 41 ppm O
Steel group: Carbon steels
Note: Precipitation diagram. Solution treated in an argon atmosphere at 1200oC (2190oF), and plunged into a tin bath for the required length of time before quenching in water. VC precipitates in ferrite as fine particles aligned in nearly parallel "rows" or lines. See the diagram No. 2785.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.
















Copyright © 2018 by Steel Data. All Rights Reserved.