0.142C-1.577Mn-0.011Nb Steel

Steel name: 0.142C-1.577Mn-0.011Nb Steel
Diagram No.: 3677
Type of diagram: CCT
Chemical composition in weight %: 0.142% C, 0.437% Si, 1.577% Mn, 0.003% S, 0.022% P, 0.024% Ni, 0.026% Cr, 0.016% Mo, 0.003% V, 0.002% Ti, 0.011% Nb, 0.017% Cu
Steel group: Microalloyed steels
Note: Austenitized at 1250oC for 3 s. See the diagrams No. 3676, No. 3678, No. 3679, No. 3680, No. 3681, No. 3682, No. 3683 and No. 3684
Note: A study of the effect of niobium in solid solution in microalloyed austenite on the kinetics of transformation to bainite after cooling.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.















Copyright © 2019 by Steel Data. All Rights Reserved.