0.30C-O.30Mn-3.64Ni-1.63Cr-O.49Mo Steel

Steel name: 0.30C-O.30Mn-3.64Ni-1.63Cr-O.49Mo Steel
Diagram No.: 3726
Type of diagram: CCT
Chemical composition in weight %: 0.30% C, 0.30% Mn, 3.64% Ni, 1.63% Cr, 0.49% Mo
Steel group: Structural steels
Note: Austenitized at 982oC. CCT diagram of a 0.1C-O.88Mn-0.34Si- 0.39Mo steel illustrating the three regions of bainite formation: points a to b, overlapping region where the 'Bs' is influenced by the prior ferrite transformation; points b to c, the plateau region where 'Bs' is almost independent of the cooling rate (the heavy line was added for emphasis); points c to d, the yielding region where bainite starts to yield to martensite.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.














Copyright © 2019 by Steel Data. All Rights Reserved.