0.97C-0.14Ni-0.14Cr-O.13Cu-0.13Si-0.16Mn Steel

Steel name: 0.97C-0.14Ni-0.14Cr-O.13Cu-0.13Si-0.16Mn
Diagram No.: 3730
Type of diagram: TTT
Chemical composition in weight %: 0.97C-0.14Ni-0.14Cr-O.13Cu-0.13Si-0.16Mn
Steel group: Hypereutectoid plain carbon steels
Note: TTT diagram of a 0.97C-0.14Ni-0.14Cr-O.13Cu- 0.13Si-0.16Mn steel showing the C-curve for the isothermal transformation of martensite. The number on the vertical axis indicates the volume percent of athermal (twinned) martensite formed during cooling to the temperatures before isothermal transformation.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

















Copyright © 2019 by Steel Data. All Rights Reserved.