0.037C-0.61Si-0.68Nb Steel

Steel name: 0.037C-0.61Si-0.68Nb
Diagram No.: 3807
Type of diagram: TTP
Chemical composition in weight %: 0.037% C, 0.61% Si, 0.68% Nb
Steel group: Creep resistant austenitic stainless steels
Note: TTP diagram from Powell et al. In their alloy (0.68Nb, 0.037C, 0.61Si wt%), G-Phase forms between 500 and 850 C, first on residual grain boundary particles of NbC, and only after very long ageing on NbC particles in the matrix. The authors propose that this is due to the easier diffusion of required elements in the grain boundaries.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.