0.32C-1.39Mn-0.33Si-0.129V-0.039Ti Steel

Steel name: 0.32C-1.39Mn-0.33Si-0.129V-0.039Ti
Diagram No.: 4034
Type of diagram: CCT
Chemical composition in weight %: 0.32% C, 1.39% Mn, 0.33% Si, 0.021% S, 0.015% P, 0.13% Cr, 0.14% Ni, 0.03% Mo, 0.129% V, 0.039% Ti, 0.129% Cu, 0.017% Sn, 0.049% Al, 148 ppm N2, 57 ppm O2, 14 ppm N free
Steel group: Carbon steels
Note: Medium carbon steel microalloyed with vanadium and titanium. CCT diagram for steel 1. The unbroken line (-) represents the conditions Tgamma=1050oC, TG=28 µm (7-8 ASTM) and the dashed line (-- -) represents the conditions, Tgamma=1250oC, TG=72 µm (4-5 ASTM).

Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.













Copyright © 2019 by Steel Data. All Rights Reserved.