1.4125 Steel

Steel name: 1.4125
Steel name of producers:
X105CrMo17 DIN EN 10088-1:2005-09 Germany
X105CrMo17 DIN EN 10088-3:2005-09 Germany
X105CrMo17 Stahl Eisen List: 2004 Germany
X105CrMo17 NF S 94-090:2001-04 Germany
N695 EXTRA Bohler Uddeholm Austria
DE4125 Dorrenberg Germany
PuroHMoExtra Hagener Gussstahlwerke Remy Germany
RM200 Kind & Co. Germany
1.4125 Platestahl Germany
1.4125 Saarstahl Germany
REMANIT4125 Thyssen Edelstahl Service GmbH Germany
ARGESTE 1.4125 YL Zapp Germany
X105CrMo17 DIN EN 10088-1:1995-08 Germany
X105CrMo17 DIN EN 10088-3:1995-08 Germany
X105CrMo17 AFNOR EN 10088-3:1995-11 France
X105CrMo17 BS EN 10088-3:1995 Great Britain
X105CrMo17 UNE EN 10088-3:1996 Spain
X105CrMo17 UNI EN 10088-1:1997 Italy
X105CrMo17 UNI EN 10088-3:1997 Italy
NIROSTA4125 ThyssenKrupp Nirosta Germany
Diagram No.: 4423
Type of diagram: CCT
Mat. No. (Wr. Nr.) designation: 1.4125
Chemical composition in weight %: 1.04% C, 0.38% Si, 0.45% Mn, 0.031% P, 0.004% S, 16.84% Cr, 0.50% Mo, 0.08% Ni, 0.11% Cu
Steel group: Stainless steels
Note: Austenitizing temperature: 1050oC, time: 15 min.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2018 by Steel Data. All Rights Reserved.