0.04C-0.2Si-2.95Mn Steel III

Steel name: 0.04C-0.2Si-2.95Mn
Diagram No.: 4935
Type of diagram: CCT
Chemical composition in weight %: See the table.
Steel group: Low carbon steels
Note: Austenitizing temperature: 800 C. Change of CCT diagrams of steel 2 with gamma grain size and the deformation in unrecrystanized gamma region.
Links: No. 4933, No. 4934 and No. 4935.
Reference: Sadahiro YAMAMOTO, et al., Effects of the Austenite Grain Size and Deformation in the uncrystallized Austenite Region on Bainite Transformation Behavior and Microstructure, ISIJ International, Vol. 35 (1 995), No. 8, pp. 1020-1026.

Transformation Diagram


Click the image to enlarge the diagram.

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2019 by Steel Data. All Rights Reserved.