0.56C-0.47Mn-0.35Si-0.10Mo-0.10Ni Steel

Steel name: 0.56C-0.47Mn-0.35Si-0.10Mo-0.10Ni
Diagram No.: 4945
Type of diagram: CCT
Chemical composition in weight %: 0.56% C, 0.47% Mn, 0.35% Si, 0.21% Cr, 0.10% Ni, 0.10% Mo
Steel group: Structural steels
Note: Calculated diagram.
Reference: L.A. Dobrzański, S. Malara, J. Trzaska, Project of computer program for designing the steel with the assumed CCT diagram, Journal of Achievements in Materials and Manufacturing Engineering, Volume 20 Issues 1-2 January-February 2007, pp. 351-354.

Transformation Diagram


Click the image to enlarge the diagram.

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.








Copyright © 2019 by Steel Data. All Rights Reserved.