0.39C-0.86Mn-0.72Cr-0.97Ni Steel

Steel name: 0.39C-0.86Mn-0.72Cr-0.97Ni
Diagram No.: 4967
Type of diagram: TTT
Chemical composition in weight %: 0.39% C, 0.86% Mn, 0.72% Cr, and 0.97% Ni
Steel group: Carbon steels
Note: Isothermal transformation diagram for a steel with 0.39% C, 0.86% Mn, 0.72% Cr, and 0.97% Ni. The upper C-shaped curves describe transformation to pearlite; the lower C-shaped curves to bainite. Ferrite is not visible. The column on the right side of the figure indicates the hardness after completed transformation measured at room temperature.
Reference: ASM Heat Treatment Volume 4, ASM International, 1991, pp. 22.

Transformation Diagram


Click the image to enlarge the diagram.

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.








Copyright © 2019 by Steel Data. All Rights Reserved.