0.081C-0.10Si-1.74Mn-0.18Ti Steel

Steel name: 0.081C-0.10Si-1.74Mn-0.18Ti
Diagram No.: 4992
Type of diagram: CCT
Chemical composition in weight %: 0.081% C, 0.10% Si, 1.74 Mn, <0.015% P, <0.015% S, 0.18% Ti
Steel group: Low carbon steels
Note: Austenitizing temperature: 1200 C/300 sec. CCT curves of the steel (a) with strain of 0; (b) with strain of 0.4.
Reference: Hai-Long YI, Lin-Xiu DU, Guo-Dong WANG and Xiang-Hua LIU, Development of a Hot-rolled Low Carbon Steel with High Yield Strength, ISIJ International, Vol. 46 (2006), No. 5, pp. 754758.

Transformation Diagram


Click the image to enlarge the diagram.

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.