AISI 1045 Steel

Steel name: AISI 1045
Diagram No.: 5001
Type of diagram: TTT
Mat. No (Wr.Nr) designation: 1.1191
SS designation: SS 1672
AFNOR designation: AFNOR XC 42 TS
AISI/SAE designation: AISI 1045
JIS designation: JIS S 45C
Chemical composition in weight %: 0.43-0.50% C, 0.60-0.90% Mn, max. 0.04% P, max. 0.05% S
Steel group: Carbon steels
Note: Time-temperature-transformation diagram of an unalloyed steel containing 0.45% C. Austenitization temperature, 880 C (1620 F). The temperature A1 is where transformation to austenite begins, and temperature A3 is where the transformation to austenite is complete.
Reference: G.E. Totten, M. Narazaki, R.R. Blackwood and L.M. Jarvis, Failures Related to Heat Treating Operation, from ASM Handbook Volume 11, Failure Analysis and Prevention (ASM International), 2002, pp. 191-193.

Transformation Diagram


Click the image to enlarge the diagram.

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.