0.28C-1.41Mn-0.29Si-0.26Cr-0.11Ni-0.22Mo-0.027Nb Steel

Steel name: 0.28C-1.41Mn-0.29Si-0.26Cr-0.11Ni-0.22Mo-0.027Nb
Diagram No.: 5009
Type of diagram: CCT
Chemical composition in weight %: 0.28% C, 1.41% Mn, 0.29% Si, 0.008% P, 0.004% S, 0.26% Cr, 0.11% Ni, 0.22% Mo, 0.20% Cu, 0.027% Nb, 0.028% Ti, 0.019% V, 0.003% B and 0.025% Al
Steel group: Nb-Ti-V microalloyed steels
Note: Austenitizing temperature: 885 C/600 sec.
Reference: M. Opiela, W. Zalecki, A. Grajcar, Influence of plastic deformation on CCT-diagrams of new-developed microalloyed steel, Journal of Achievements in Materials and Manufacturing Engineering, Volume 51 Issue 2 April 2012, pp. 78-89.

Transformation Diagram


Click the image to enlarge the diagram.

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.