0.38C-0.64Mn-0.23Si-0.99Cr Steel

Steel name: 0.38C-0.64Mn-0.23Si-0.99Cr
Diagram No.: 5035
Type of diagram: CCT
Chemical composition in weight %: 0.38% C, 0.64% Mn, 0.23% Si, 0.99% Cr, 0.08% Ni, Mo (see the diagram)
Steel group: Structural steels
Note: Austenitizing temperature: 850 C. Effect of molybdenum on CCT diagram shape of the steel austenitized at the temperature of 850°C with concentrations: 0.38%C, 0.64%Mn, 0.23%Si, 0.99%Cr, 0.08%Ni.
Reference: W. Sitek, J. Trzaska, Numerical simulation of the alloying elements effect on steels’ properties, Journal of Achievements in Materials and Manufacturing Engineering, Volume 45 Issue 1 March 2011, pp. 71-78.

Transformation Diagram


Click the image to enlarge the diagram.

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.