60NiCrMo11-03 Steel

Steel name: 60NiCrMo11-03
Diagram No.: 5054
Type of diagram: CCT
Chemical composition in weight %: 0.57 % C, 2.36 % Ni, 0.75 % Cr , 0.41 % Mo
Steel group: Structural steels
Note: Austenitizing temperature: 850 C/30 min. A-Austenite, C-Cementite, c-Carbides, F-Ferrite, M-Martensite.
Reference: Guy MURRY, Transformations dans les aciers, Techniques de l’Ingénieur, traité Matériaux métalliques, Doc. M 1 115 - 5, 1999, pp. 1-54.

Transformation Diagram


Click the image to enlarge the diagram.

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2019 by Steel Data. All Rights Reserved.