0.038C-0.25Si-1.43Mn-17.50Cr-12.81Ni-4.60Mo-0.55Nb Steel

Steel name: 0.038C-0.25Si-1.43Mn-17.50Cr-12.81Ni-4.60Mo-0.55Nb
Diagram No.: 5132
Type of diagram: TTP
Chemical composition in weight %: 0.038% C, 0.25% Si, 1.43% Mn, 0.018% P, 0.012% S, 17.50% Cr, 12.81% Ni, 4.60% Mo, 0.55% Nb
Steel group: Austenitic stainless steels
Note: The three intermetallic phases discussed above can occur together in molybdenum-alloyed austenitic steels. The order of formation, the range of stability and the relative amounts are, however, very sensitive to the chemical composition and possibly also to the solution treatment preceeding the precipitation heat treatment. This is shown for example in the time-temperature-precipitation diagrams in Diagram No. 5130, Diagram No. 5131, Diagram No. 5132, and Diagram No. 5133.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.














Copyright © 2019 by Steel Data. All Rights Reserved.