0.35%C-0.23Si-0.65Mn-1.11Cr-0.05Mo-0.23Ni-0.11Cu Steel

Steel name: 0.35%C-0.23Si-0.65Mn-1.11Cr-0.05Mo-0.23Ni-0.11Cu
Diagram No.: 5159
Type of diagram: CCT
Chemical composition in weight %: 0.35% C, 0.23% Si, 0.65% Mn, 1.11% Cr, 0.05% Mo, 0.23% Ni, 0.11% Cu
Steel group: Structural steels, low alloy steels
Note: CCT diagram and calculated cooling curves. Figure corresponds to the CCT diagram for the steel evaluated1 where are also plotted some calculated cooling curves considering each investigated welding condition in this study. The cooling curves have started from a local at the HAZ where the peak temperature has reached about 1100 C, with the volume fraction of the constituents and the hardness indicated in Figure, calculated using the mathematical formulation presented in this study.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.















Copyright © 2019 by Steel Data. All Rights Reserved.