0.079C-1.39Mn-0.20Si-0.002Al-0.012Ti Steel

Steel name: 0.079C-1.39Mn-0.20Si-0.002Al-0.012Ti
Diagram No.: 5203
Type of diagram: CCT
Chemical composition in weight %: 0.079% C, 1.39% Mn, 0.20% Si, 0.0007% P, 0.0007% S, 0.002% Al, 0.012% Ti, 0.001595% N, 0.001796% O
Steel group: Welding steels
Note: CCT curves of a Ti killed steel (heating temperature 1400 C (Yamamoto et al. 1989) (Fp = grain boundary ferrite, F1 = polygonal ferrite, IFPI = acicular ferrite, type I, IFPII = acicular ferrite, type II, P = pearlite, PL = degenerated pearlite, B = bainite and M = martensite). Welding CCT diagram.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.
















Copyright © 2019 by Steel Data. All Rights Reserved.