0.05C-1.7Mn-0.10Nb-0.10Mo-0.25Cr Steel

Steel name: 0.05C-1.7Mn-0.10Nb-0.10Mo-0.25Cr
Diagram No.: 5226
Type of diagram: CCT
Chemical composition in weight %: 0.04% C, 1.4% Mn, 0.10% Nb, 0.30% Mo. 0.05% C, 1.7% Mn, 0.10% Nb, 0.10% Mo, 0.25% Cr. 0.05% C, 1.6% Mn, 0.10% Nb, 0.20% Ni, 0.25% Cu, 0.25% Cr.
Steel group: HSLA steels
Note: Transformation behavior of various low-carbon alloys of similar Pcm and strength level (holding at 1200C for 10 minutes, deformation = 0.6 at 1050C, deformation = 0.6 at 850C, cooling at various rates).
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.