0.094C-0.30Si-1.32Mn Steel

Steel name: 0.094C-0.30Si-1.32Mn
Diagram No.: 5326
Type of diagram: CCT
Chemical composition in weight %: 0.094% C, 0.30% Si, 1.32% Mn
Steel group: Welding steels
Note: Welding diagram. CCT diagrams. (a) FG HAZ (b) GC HAZ (c) WM.
There are two variants of CCT diagrams, one is for thermal processing, and the other is for welding. In TMCP of steel precise control of the microstructure necessitates accurate application of accelerated cooling. In welding, understanding the relationship between the cooling rate and the microstructure in both the HAZ and the weld metal is critical to maintaining high integrity joints. In both cases, the CCT diagram is a reflection of the shift from equilibrium transformation predicted by the phase diagram under non-equilibrium cooling conditions. The different types of CCT diagrams and their application to the GC HAZ, FG HAZ and the weld metal are illustrated in Figure.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.












Copyright © 2019 by Steel Data. All Rights Reserved.