~X50CrMoW9-1-1 Steel

Material designation: ~X50CrMoW9-1-1
Diagram No.: 242
DIN designation: ~X50CrMoW9-1-1
Mat.No. (Wr.Nr.) designation: ~1.2631
Chemical composition in weight %: 0.53% C, 0.50% Si, 0.30% Mn, 7.50% Cr, 1.60% Mo, 1.50% W
Steel group: Cold work tool steels
Applications: Highly stressed machine knives for the cellulose, paper and fiberboard industries, and circular shears for plate of up to 15 mm thickness
Comment: No data
Source: HTDHK, 2008

Heat Treatment
Hardening: 1000 to 1020oC/oil, 1020 to 1040oC/air
Tempering: See the diagram
Note: Diagram: specimen size: square 20 mm. Hardening temperature: 1010oC.

Tempering Diagram

Price: 25.00 US $
Buy Online