Nickel deposits on steel - Chemical etching

Material Name: Nickel deposits on steel
Recipe No.: 10525
Primary Chemical Element in Material: Fe
Sample Type: Bulk
Uses: General microstructure
Etchant Name: None
Type (Macro/Micro): Micro
Etching Method: Chemical
Etchant (Electrolyte) Composition: 1 part HNO3, 4 parts acetic acid.
Procedure (Condition): No data
Note: Coatings on steels. For nickel deposits on steel. Reveals structure of nickel.
Reference: Vander Voort, Metallography Principles and Practice, McGraw-Hill, Inc., 1984, p. 637.