Magnesia (MgO) - Chemical etching

Material Name: Magnesia (MgO)
Recipe No.: 4164
Primary Chemical Element in Material: Mg
Sample Type: Bulk
Uses: General microstructure
Etchant Name: None
Type (Macro/Micro): Micro
Etching Method: Chemical
Etchant (Electrolyte) Composition: Solution of ammonium chloride and sulphuric acid.
Procedure (Condition): No data
Note: No data
Reference: J.H.Greiner, et al., J.App.Phys., Vol.37, No.5, April 1966, p. 2149.