Aqua Regia - Molybdenum - Chemical etching

Material Name: Molybdenum
Recipe No.: 4203
Primary Chemical Element in Material: Mo
Sample Type: Bulk
Uses: General microstructure
Etchant Name: Aqua Regia
Type (Macro/Micro): Micro
Etching Method: Chemical
Etchant (Electrolyte) Composition: Aqua Regia
Procedure (Condition): No data
Note: No data
Reference: B.J.Shaw, J.Less Comm.Metals, Vol.13, No.3, September 1967, p. 294.