Sn-Sb-Pb alloys - General macrostructure

Material Name: Sn-Sb-Pb alloys
Recipe No.: 9632
Primary Chemical Element in Material: Sn
Sample Type: Bulk
Uses: General macrostructure
Etchant Name: None
Type (Macro/Micro): Macro
Etching Method: Chemical
Etchant (Electrolyte) Composition: 1 ml silver nitrate, 99 ml H2O.
Procedure (Condition): Etch by immersion of sample. Rub smut off under running water.
Note: No data
Reference: Vander Voort, Metallography Principles and Practice, McGraw-Hill, Inc., 1984, p. 529.