Etchants for Nickel and Alloys

18/8 Stainless steels - Etching for delta ferrite
68Ni-31.9Fe-0.1Mg and 63Ni-35Fe-2Mo single crystals - Chemical etching
718 alloy - Ni-0.03C-19Cr-3Mo-18Fe-0.6Al-1Ti-5Nb+Ta
79Ni-17Fe-44Mo (111) oriented Permalloy wafers - Electrolytic polishing
79Ni-17Fe-4Mo Permalloy single crystal specimens - Chemical polishing
AG-21's etchant for superalloy - Chemical etching
ASTM etchant No. 10 - Ni superalloys - Chemical etching
ASTM etchant No. 105 - Ni superalloys - Chemical etching
ASTM etchant No. 107 - Ni superalloys - Electrolytic etching
ASTM etchant No. 107 - Ni superalloys - Electrolytic etching
ASTM etchant No. 107 - Ni-Fe alloys - Electrolytic etching
ASTM etchant No. 108 - Pure Ni and high Ni alloys - Electrolytic etching
ASTM etchant No. 111 - Ni superalloys - Chemical etching
ASTM etchant No. 12 - Ni superalloys - Chemical etching
ASTM etchant No. 133 - Ni superalloys - Chemical etching
ASTM etchant No. 133 - Ni-Ti
ASTM etchant No. 133 - Ni-Ti alloys - Chemical etching
ASTM etchant No. 134 - Ni-Cr
ASTM etchant No. 134 - Ni-Cr alloys - Electrolytic etching
ASTM etchant No. 134 - Ni-Fe alloys - Electrolytic etching
ASTM etchant No. 134 - Pure Ni and high Ni alloys - Electrolytic etching
ASTM etchant No. 135 - Pure Ni and high Ni alloys
ASTM etchant No. 135 - Pure Ni and high Ni alloys - Chemical etching
ASTM etchant No. 136 - Pure Ni and high Ni alloys
ASTM etchant No. 136 - Pure Ni and high Ni alloys - Chemical etching
ASTM etchant No. 137 - Pure Ni and high Ni alloys
ASTM etchant No. 137 - Pure Ni and high Ni alloys - Electrolytic etching
ASTM etchant No. 138 - Carapella's etchant - Ni-Ag
ASTM etchant No. 138 - Ni superalloys - Chemical etching
ASTM etchant No. 138 - Ni-Ag alloys - Chemical etching
ASTM etchant No. 139 - Ni-Ag
ASTM etchant No. 139 - Ni-Ag alloys - Chemical etching
ASTM etchant No. 13a - Ni superalloys - Electrolytic etching
ASTM etchant No. 13a - Ni-Cr alloys - Electrolytic etching
ASTM etchant No. 140 - Ni-Al
ASTM etchant No. 140 - Ni-Al alloys - Chemical etching
ASTM etchant No. 140 - Ni-Fe alloys - Chemical etching
ASTM etchant No. 141 - Contrast etchant - Ni-Al
ASTM etchant No. 141 - Ni-Al alloys - Chemical etching
ASTM etchant No. 141 - Ni-Fe alloys - Chemical etching
ASTM etchant No. 142 - Ni-Al
ASTM etchant No. 142 - Ni-Al alloys - Electrolytic etching
ASTM etchant No. 143 - Ni-Al
ASTM etchant No. 143 - Ni-Al alloys - Chemical etching
ASTM etchant No. 143 - Ni-Ti alloys - Chemical etching
ASTM etchant No. 144 - Ni-Cr
ASTM etchant No. 144 - Ni-Cr alloys - Electrolytic etching
ASTM etchant No. 145 - Ni-Cr
ASTM etchant No. 145 - Ni-Cr alloys - Electrolytic etching
ASTM etchant No. 146 - Ni-Cr
ASTM etchant No. 146 - Ni-Cr alloys - Chemical etching
ASTM etchant No. 147 - Ni-Cr
ASTM etchant No. 147 - Ni-Cr alloys - Chemical etching
ASTM etchant No. 148 - Ni-Fe
ASTM etchant No. 148 - Ni-Fe alloys - Chemical etching
ASTM etchant No. 149 - Ni-Fe
ASTM etchant No. 149 - Ni-Fe alloys - Chemical etching
ASTM etchant No. 150 - Ni-Fe
ASTM etchant No. 150 - Ni-Fe alloys - Chemical etching
ASTM etchant No. 151 - Ni-Ti
ASTM etchant No. 151 - Ni-Ti alloys - Chemical etching
ASTM etchant No. 152 - Ni-Zn
ASTM etchant No. 152 - Ni-Zn alloys - Chemical etching
ASTM etchant No. 153 - Ni superalloys
ASTM etchant No. 153 - Ni superalloys - Chemical etching
ASTM etchant No. 154 - Ni superalloys
ASTM etchant No. 154 - Ni superalloys - Chemical etching
ASTM etchant No. 154 - Ni superalloys - Chemical etching
ASTM etchant No. 155 - Beraha's E etchant - Ni superalloys
ASTM etchant No. 155 - Ni superalloys - Chemical etching
ASTM etchant No. 156 - Ni superalloys - Electrolytic etching
ASTM etchant No. 157 - Hastelloy-W - Chemical etching
ASTM etchant No. 157 - Ni Hastelloy-W
ASTM etchant No. 18 - Ni superalloys - Electrolytic etching
ASTM etchant No. 19b - Ni superalloys - Chemical etching
ASTM etchant No. 21 - For high temperature alloys
ASTM etchant No. 22 - HCl+H2O2 - For high temperature alloys
ASTM etchant No. 22a - Ni superalloys - Chemical etching
ASTM etchant No. 24 - HCl-HNO3-FeCl3 - For high temperature alloys
ASTM etchant No. 25 - Marble's etchant - For high temperature alloys
ASTM etchant No. 25 - Ni superalloys - Chemical etching
ASTM etchant No. 25 - Ni-Fe alloys - Chemical etching
ASTM etchant No. 25 - Pure Ni and high Ni alloys - Chemical etching
ASTM etchant No. 31c - Pure Ni and high Ni alloys - Electrolytic etching
ASTM etchant No. 38 - Ni-Ag alloys - Chemical etching
ASTM etchant No. 40 - Ni-Fe alloys - Chemical etching
ASTM etchant No. 47 - Pure Ni and high Ni alloys - Chemical etching
ASTM etchant No. 50 - Ni-Ag alloys - Chemical etching
ASTM etchant No. 50 - Ni-Al alloys - Chemical etching
ASTM etchant No. 50 - Ni-Cr alloys - Chemical etching
ASTM etchant No. 50 - Ni-Fe alloys - Chemical etching
ASTM etchant No. 50 - Ni-Ti alloys - Chemical etching
ASTM etchant No. 74e - Ni-Fe alloys - Chemical etching
ASTM etchant No. 74e - Ni-Mn alloys - Chemical etching
ASTM etchant No. 83 - Ni-Cr alloys - Electrolytic etching
ASTM etchant No. 83 - Ni-Fe alloys - Electrolytic etching
ASTM etchant No. 89 - Ni-Al alloys - Chemical etching
ASTM etchant No. 94 - Ni superalloys - Chemical etching
ASTM etchant No. 98 - Ni-Cr alloys - Chemical etching
Adler's etchant - Ni alloys - General macrostructure
Adler's etchant - Ni brazing alloys when brazed to steels - Galvanic Ni coatings - Chemical etching
Adler's etchant - Ni-base foundary alloys - Chemical etching
Agua Regia - Ni alloys - General macrostructure
Agua Regia - Ni superalloys, Ni-Cr alloys - Chemical etching
Agua Regia - Ni-Cr thin films evaporated on (111) and (100) oriented Si - Chemical etching
Agua Regia, modified - Ni specimens - Chemical etching
Al-Ni alloy - Al-Al3Ni eutectic
Alloy 800 - 0.04/0.05C-0.2/0.5Si-0.5/0.6Mn-33/34.5Ni-21.5/22.5Cr-0.2/0.55Ti-0.1/0.2Al-0/0.1Cu
Alloy Fe47Ni44Al9 - Twin jet polishing mehod
Alloy MA 6000 - Twin jet polishing mehod
Alloy Ni33Al33Cr34 - Twin jet polishing mehod
Alloy Ni50Al50 - Twin jet polishing mehod
Alloy Ni50Co18Al32 - Twin jet polishing mehod
Alloy Ni74Al25C1 - Twin jet polishing mehod
Alloy Ni76Al17Ti6 - Twin jet polishing mehod
Alloy Ni89Al11 - Twin jet polishing mehod
Alloy NiAl - Electrolytic polishing
Alloy SRR99 - Twin jet polishing mehod
Alloys containing Cr, Fe, and other elements I - Chemical etching - General macrostructure
Alloys containing Cr, Fe, and other elements III - Chemical etching - General macrostructure
Alloys containing Cr, Fe, and other elements IV - Chemical etching - General macrostructure
Alumel alloy - 95Ni-1.6Al-1.5Si-1.3Mn-0.3Co
Alumina dispersed Nichrome - Ni-20% Cr-0.6/1.5% Al2O3 - Electrolytic thinning
Aluminia-lanthanum oxide dispersed Nichrome - Ni-20Cr-0.04Al2O3-0.04La2O3
Aqua Regia - Ni and Ni alloys
Aqua Regia - Ni-Cr-Fe alloys (Inconel) - Chemical etching
Astraloy - Ni-16/18Co-15/16Cr-4.5/5.5Mo-3.85/4.15Al-3.35/3.65Ti-0.03/0.09C (+B)
B1900 alloy - Ni-8Cr-6Mo-1Ti-6Al-10Co-4Ta-0.1C (+B, Zr)
Beraha's E etchant - Ni superalloys
Beraha's III I etchant - Ni-base alloys, Hastelloy X, Hastelloy
Beraha's III etchant - Ni base casting alloys - Chemical etching
Beraha's III etchant - Ni-base alloys with more than 9Mo, Hastelloy X, Hastelloy C - Chemical etching
Beraha's tint etchant - Ni superalloys - Tint etching
Beraha's tint etchant - Ni-base alloys
CMSX-6 alloy - Electrolytic polishing
Canada's etchant - Nickel superalloy 718 - Chemical etching
Carapella's etchant - Ni and Ni-Cu (Monel) alloys - Chemical etching
Carpella's etchant - Ni-B alloys - Chemical etching
Coated Hastelloy-X - Chemical etching
Color etching Ni-Cr alloys - Chemical etching
Contrast etchant - Ni-Al alloys
Cr carbide-Ni alloy - 83% carbide-15% Ni
E etchant - Ni superalloys
Electroless Ni - For revealing the grain structure
Electroless nickel 1 plating
Electroless nickel 2 plating
Electrolytes for TEM preparation od intermetallics
Electrolytic nickel plating
Electrolytic polishing NiTi alloys
Etch pits etchant - Nickel oxide (NiO)
Etchants for Inconel-X alloy
Etching Rene 80 alloy - Electrolytic etching
Evans etchant - Inconel 617 - Chemical etching
Extraction replica etchant for nickel alloys - Chemical etching
Fe-Ni alloys - Chemical etching
Fe-Ni oxide couple - Chemical etching
Fe-Ni thin film - Chemical cleaning
Flat's etchant - Ni-Ti alloys
Fry's etchant - Ni-Ge alloys - Chemical etching
Fry's etchant - Ni-Pd-Ga alloys - Chemical etching
Fry's etchant - Ni-Pt-Ga alloys - Chemical etching
Fry's etchant - Nimonic alloys - Nimonic alloys PE7, PE11, and PE16, Nimonic Pk 31
GTD-111 alloy etching
Gamma-prime-age hardening, Ni-base alloys, grain-boundaries etch - Chemical etching
Glyceregia - Ni superalloys and Ni-Cr alloys - Chemical etching
HAFNIC 10 alloy - Ni-10Cr-5Al-5Co-8.3Hf-1.1Zr-0.7C
Hastelloy B, B2, B3, N, and W alloys - Chemical etching
Hastelloy W - Chemical etching
Hastelloy X - Chemical etching
Hastelloy X - Chemical etching
Hastelloy X - Electrolytic etching
Hastelloy X - Ni-22Cr-18.5Fe-9Mo-0.6W
Hastelloy X etching - Electrolytic etching
Hastelloy and Haynes alloys - Electrolytic etching
Hasteloy B - Ni-28Mo-1Fe-0.7Cr+C
Hayness No. 21 alloy - Electrolytic etching
Hayness No. 21 alloy - Electrolytical etching
Hayness No. 25 alloy - Shows magnetic domain
Hayness No. 30, X40 alloys - Electrolytic etching
Hayness No. 36 alloy - Electrolytic etching
Heat resisting alloy - One of the best electrolyte for universal use
Heppenstall etchant - Ni-based superalloys - General macrostructure
Heppenstall's etchant - Inconel 625 alloy - Chemical etching
High Ni-alloys - General macrostructure
High temperature nickel alloys - Chemical and Electrolytic etching
High-Ni alloys - Chemical etching - General macrostructure
High-temperature alloys - Electrolytic polishing
IN 100 alloy - 56.1Ni-5.0Al-4.5Ti-12Cr-3.2Mo-18.4Co-0.8V-0.09C (+B) by weight
IN 738 alloy - Electrolytic-potentiostatic isolation of residues
IN 738 alloy - Sample preparation
In-738 superalloy - Ni-0.2C-3.5Al-3.6Ti-8.4Co-15.75Cr-1.7Mo-0.9Nb-1.8Ta-2.8W
Inco 713LC superalloy - Electrolytic etching
Inconel - Electrolytic polishing
Inconel 600 - Chemical etching
Inconel 617 - 54Ni-22Cr-12.5Co-9Mo-1Al-0.07C
Inconel 625 - Chemical etching
Inconel 625 - Chemical etching
Inconel 686 - Chemical etching
Inconel 690 - Chemical etching
Inconel 718 - For SEM examination to view gamma double prime in alloy 718 (no gamma prime)
Inconel 718 - Ni-0.5Al-0.05C-5Nb-0.2/0.4Co-18Cr-18/20Fe-3Mo
Inconel 718 - Ni-17Cr-22Fe-1Co-5Nb-0.8Ti-0.6Al-0.05C
Inconel 718 alloy - Chemical etching
Inconel X550, Inco 700, Waspaloy, M252 - Chemical etching
Inconel X550, Inco 700, Waspaloy, and M252 - Chemical etching
Jewitt-Wise's etchant - Ni specimens - Chemical etching
Kalling's 2 etchant - Ni-Cu alloys and Ni-base superalloys - Chemical etching
Kalling's etchant - Nickel specimens T.D. grade - Chemical etching
Kalling's etchant - Wrought Fe-Ni-Cr heat resisting alloy - U-700 (AISI 687) - General structure
Kallings 2 etchant - Ni-Cu alloys and superalloys - Chemical etching
Keller' etchant, modified - Ni-Cr-Th alloy - Ni-20Cr-2ThO2
Klemm's III etchant - Ni alloys - Tint etching
Kovar alloy - Electrolytic etching
Lenoir's solution - Nimonic PE16 alloy
Lepito's No. I etchant - Ni alloys - General macrostructure
Lepito's No. II etchant - Ni-Cr-Fe alloys - General macrostructure
Lepito's etchant - Ni and its alloys - Alloys containing Cr, Fe and other elements - Etchant for nickel welds
Lepito?s etchant II - Alloys containing Cr, Fe, and other elements II - Chemical etching
Lithia dispersed Nichrome (Cr-Li-Ni-O)-Ni-20Cr-1.3Li2O
Livingstone's solution - For Ni - Electrolytic polishing
Low Ni alloys - General macrostructure
Low-Ni alloys - Chemical etching - General macrostructure
Lucas's etchant - Ni3Al based alloys with 21-29 at. per cent Al - Chemical etching
Lucas's etchant - NiChrome 80-20 - Grain structure and matrix phases
MA 956E alloy - Fe-19Cr-4.4Al-0.5Ti-0.4Ni-0.5Y2O3
MAR-M 509 alloy - Chemical etching
MCrAlY-coatings (NiCoCrAlY coating) - Chemical etching
MERL 76 alloy - 55Ni-5.1Al-4.2Ti-12Cr-3.3Mo-0.02C-18.4Co-1.3Nb-0.7Hf (+B)
MP35N alloy - Chemical etching
Mar M247 - Electrolytic polishing
Marble's etchant - Ni and its alloys - Nickel - For grain structure
Marble's etchant - Ni, Ni-Cu and Ni-Fe alloys and superalloys - Chemical etching
Marble's etchant - Ni-Cr alloys - Chemical etching
Marble's etchant - Ni-Cr-Th alloy - Etch for TD Ni-Cr
Marble's etchant - Ni-Mo-Cr-Si alloy - 50Ni-31Mo-15Cr-3Si
Marble's etchant - Nickel - Attack polishing
Marble's etchant - Nickel - General macrostructure
Marble's etchant - Nickel superalloy 718 - Chemical etching
Marble's etchant - Nickel superalloys - Production of thin foils for electron microscopy
Marble's etchant - Wrought Fe-Ni-Cr heat resisting alloy - U-700 (AISI 687) - Good for contrast
Marble's etchant, modified - For Ni-Nb alloys
Marble's etchant, modified - Ni alloys - General macrostructure
Marble's etchant, modified - Ni and its alloys - Alloys containing Cr, Fe and other elements
Marble?s etchant - Nickel - Chemical etching - General macrostructure
Monel 400 - For the grain boundaries
Monel, Ni-Al and Ni-Fe alloys - Chemical etching
Murakami's etchant - Ni-Cu alloys and superalloys - Chemical etching
Murakami's etchant - Wrought Fe-Ni-Cr heat resisting alloys - Inconel 706 and alloy 718, carbide particles
NASA 11B7 alloy - 56.6Ni-3.4Al-0.7Ti-8.9Cr-2.0Mo-0.1C-9.1Co-7.5W-0.5V-10.2Ta-1.1Hf (+ 0.02 B) by weight
Nb and Nb alloys - Electrolytic polishing
Nb and Nb alloys - Electrolytic polishing
New etching procedure for Ni alloy 690
Ni (100) wafers - Chemical etching
Ni (100) wafers - Ionized gas cleaning
Ni alloy - XRD sample preparation
Ni alloy - XRD sample preparation
Ni alloy - XRD sample preparation
Ni alloy - XRD sample preparation
Ni alloy - XRD sample preparation
Ni alloys - Chemical etching
Ni alloys, some alloy steels - Attack polishing
Ni and Ni alloys - Electrolytic polishing
Ni and Ni alloys - Electrolytic polishing
Ni and Ni alloys - Electrolytic polishing
Ni and Ni alloys - Electrolytic polishing
Ni and Ni alloys - Electrolytic polishing
Ni and Ni alloys - Electrolytic polishing
Ni and Ni alloys - Electrolytic polishing
Ni and Ni alloys - Electrolytic polishing
Ni and Ni alloys - Electrolytic polishing
Ni and Ni alloys - Electrolytic polishing
Ni and Ni alloys - General macrostructure
Ni and Ni alloys - General macrostructure
Ni and Ni-Cu alloys - Electrolytic etching
Ni and alloys - Chemical etching
Ni and its alloys - Alloys containing Cr, Fe and other elements
Ni and its alloys - Alloys containing Cr, Fe and other elements - Grain structure
Ni and its alloys - High Ni alloys - Porosity and flow lines
Ni and its alloys - Low Ni alloys - Grain structure
Ni crystalline electrode rod - Alcohol cleaning
Ni evaporated as an AuNi coating on resistors - Chemical etching
Ni evaporated thin films - Chemical etching
Ni passive superalloys - Chemical etching
Ni polycrystalline specimens - Electrolytic etching
Ni silicide - Chemical etching
Ni single crystal sphere - Thermal forming
Ni single crystals - Electrolytic thinning
Ni specimens - Chemical cleaning
Ni specimens - Chemical cleaning
Ni specimens - Chemical etching
Ni specimens - Chemical etching
Ni specimens - Chemical etching
Ni specimens - Chemical polishing
Ni specimens - Chemical polishing
Ni specimens - Electrolytic etching
Ni specimens - Electrolytic polishing
Ni specimens - Electrolytic polishing
Ni specimens - Electrolytic polishing
Ni specimens - Electrolytic polishing
Ni specimens - Electrolytic polishing
Ni superalloys - Chemical etching
Ni superalloys - Chemical etching
Ni superalloys - Chemical etching
Ni superalloys - Chemical etching
Ni superalloys - Chemical etching
Ni superalloys - Chemical etching
Ni superalloys - Electrolytic etching
Ni superalloys - Electrolytic etching
Ni superalloys - Electrolytic etching
Ni superalloys - Electrolytic etching
Ni superalloys - Electrolytic etching
Ni superalloys, Hastelloy - Chemical etching
Ni thin film evaporation on glass - Chemical etching
Ni thin films - Chemical etching
Ni, 20% Cr and 2% ThO2 alloy - Electrolytic etching
Ni, Ni-Cr and Ni-Fe alloys - Electrolytic etching
Ni, Ni-Cu, Ni-Ti alloys - Chemical etching
Ni-20Cr and Ni-20Cr-45Fe - Chemical etching
Ni-Ag alloys - Chemical etching
Ni-Ag alloys and superalloys - Chemical etching
Ni-Ag, Ni-Al, Ni-Cr, Ni-Cu, Ni-Fe and Ni-Ti alloys - Electrolytic etching
Ni-Al alloy - 70Ni-30Al
Ni-Al alloy - Al-Al3Ni eutectic
Ni-Al alloy - Al-Al3Ni eutectic
Ni-Al alloy - Al-Al3Ni eutectic
Ni-Al alloy - Al-Al3Ni eutectic
Ni-Al alloy - Al-Al3Ni eutectic
Ni-Al alloy - Al-NiAl3 eutectic
Ni-Al alloy - Alloy with 0.1-0.5 at.% Al
Ni-Al alloy - Alloy with 4-8% Al
Ni-Al alloy - Beta type alloys
Ni-Al alloy - Electrolytic thinning
Ni-Al alloy - Electrolytic thinning
Ni-Al alloy - Electrolytic thinning
Ni-Al alloy - Electrolytic thinning
Ni-Al alloy - Electrolytic thinning
Ni-Al alloy - Ni rich NiAl - Electrolytic polishing
Ni-Al alloy - Ni-6/8Al - Electrolytic polishing
Ni-Al alloy - Ni3Al
Ni-Al alloys (3-25% Al) - Chemical etching
Ni-Al alloys - Chemical etching
Ni-Al alloys - Chemical etching
Ni-Al alloys - Chemical etching
Ni-Al alloys - Electrolytic polishing
Ni-Al system - Al-Al3Ni eutectic - Electrolytic polishing
Ni-Al system - Chemical etching
Ni-Al, Ni-Cr-Al and Ni-Cr-Ti alloys - Electrolytic etching
Ni-Al-Cu steel - Fe-0.3C-4Ni-1Al-1Cu
Ni-Al-Hf alloy - Ni-20/23Al-5/7.5Hf
Ni-Al-Mo alloy - 65Ni-8Al-27Mo
Ni-Al-Mo alloy - Ni-8Al-26.4Mo, Ni-6.3Al-31.2Mo
Ni-Al-Mo alloy - NiAl/Mo eutectic - Selective etch for Mo
Ni-Al-Mo alloy - Ternary eutectic of gama prime-Ni3Al, gamma-nickel rich f.c.c and alpha-Mo
Ni-Al-Nb alloy - Ni rich alloys
Ni-Al-Nb alloy - Ni3Al-Ni3Nb eutectic
Ni-Al-Ta alloy - Ni-20/29Al-2.5/7.5Ta
Ni-Al-Ti alloy - Ni3(Al,Ti) - Electrolytic thinning
Ni-Al-Ti alloy - Ni3AlTi - Electrolytic polishing
Ni-Al-Ti alloy - Ni3AlTi, etch pits
Ni-Al-Ti alloys - Electrolytic etching
Ni-B-P glass - Ni80-P10-B10 splat cooled alloy
Ni-B-Si-C alloy - Electrolytic polishing
Ni-Be-Cr alloys - Electrolytic thinning
Ni-C alloys - Chemical etching
Ni-Chrome - Electrolytic polishing
Ni-Chrome - Electrolytic polishing
Ni-Co (15%) specimens - Electrolytic thinning
Ni-Co alloy - Alloy with 32 at.% Ni
Ni-Co alloy - Electrolytic thinning
Ni-Co alloy - Electrolytic thinning by window technique
Ni-Co-Al alloys - Electrolytic polishing and etching
Ni-Co-Cr alloy - 29-34 wt.% Ni, 30-34 wt.% Co, 32-41 wt.% Cr
Ni-Co-Cr alloy - 29-34 wt.% Ni, 30-34 wt.% Co, 32-41 wt.% Cr
Ni-Co-Cr-Mo alloy - 30-32 wt.% Ni, 30-32 wt.% Co, 34 wt.% Cr, 2-7 wt.% Mo
Ni-Co-Cr-Mo alloy - 30/32 wt.% Ni-30/32 wt.% Co-34/30 wt.% Cr-1/7 wt.% Mo
Ni-Co-Cr-W alloy - 28-32 wt.% Ni, 28-32 wt.% Co, 32-34 wt.% Cr, 2-11 wt.% W
Ni-Co-Cr-W alloy - 28-32 wt.% Ni-28-32 wt.% Co-32-34 wt.% Cr-2-11 wt.% W
Ni-Co-Ti alloy - Ti4Co3Ni
Ni-Cr specimens - Electrolytic polishing
Ni-Cr alloy - Alloys with < 20% Cr
Ni-Cr alloy - Alloys with 10-12% Cr
Ni-Cr alloy - Electrolytic polish and etching
Ni-Cr alloy - Electrolytic thinning by window technique
Ni-Cr alloy - Ni2Cr - Electrolytic polishing
Ni-Cr alloy - Preferential electrolytic polishing for chromium rich phases
Ni-Cr alloys - Chemical etching
Ni-Cr alloys - Chemical etching
Ni-Cr alloys - Electrolytic etching
Ni-Cr alloys - Electrolytic etching
Ni-Cr alloys - Electrolytic etching
Ni-Cr alloys - Electrolytic etching
Ni-Cr alloys - Electrolytic etching
Ni-Cr as an evaporated thin film on (100) oriented Si wafers - Chemical etching
Ni-Cr evaporated thin films on (100) Si wafers - Chemical etching
Ni-Cr matrix - TaC wire composite-Shows up fibre shape and facets (111) planes in FCC matrix
Ni-Cr residual metals - Chemical cleaning
Ni-Cr specimens - Chemical etching
Ni-Cr specimens - Electrolytic cutting
Ni-Cr specimens - Electrolytic thinning
Ni-Cr thin film deposition as a bimetallic layer of Au/Ni-Cr - Chemical etching
Ni-Cr-Al alloy - 82Ni-12Cr-6Al - Electrolytic polishing
Ni-Cr-Al alloy - Electrolytic thinning by window technique
Ni-Cr-Al alloy - Ni-Al/Cr eutectic
Ni-Cr-Al alloy - NiAl/Cr eutectic
Ni-Cr-Al alloy - NiAl0Cr eytectic 33 at.% Ni, 33 at.% Al, 34 at.% Cr
Ni-Cr-Al alloys - Chemical etching
Ni-Cr-Al-C alloy - Ni-15Cr-3/10Al-0.05/0.3C
Ni-Cr-Al-Mo alloy - (NiAl-Cr(Mo)) eutectic
Ni-Cr-Al-Mo-Nb-Ti-Zr alloy - Inco 713LC Ni-12Cr-6Al-0.8Ti-4.6Mo-1.5/2.5Nb-0.1Zr-(+C,B)
Ni-Cr-Al-Ta alloy - Ni-16Cr-5Al-4Ta - Reveals gama prime precipitates
Ni-Cr-Al-Ti alloy - 10-12 Cr, 5-6 Ni, 1 Ti
Ni-Cr-Al-Ti alloy - In 853 or Inconel MA 753, Ni-19Cr-1.2Al-2.4Ti (+Zr, B, Y2O3)
Ni-Cr-Al-Ti alloy - Ni-15Cr-3(Ti+Al), Ni-20Cr-3(Ti+Al), Ni-20Cr-4(Ti+Al)
Ni-Cr-Al-Ti alloy - Ni-4/13Al-6.5/20.5Cr-0.25/4.75Ti (at.%)
Ni-Cr-Al-Ti-C alloy - 10-12% Cr, 5-6% Al, 1% Ti, 0.1% C
Ni-Cr-Al-Ti-C alloy - Ni-15Cr-1/4.5Al-2.5/6Ti-0.15/0.25C
Ni-Cr-Al-Ti-Ta alloy - 10-12 Cr, 5-6 Al, 1 Ti, 0.15 Ta
Ni-Cr-Al-Ti-Ta-C alloy - 10/12Cr-5/6Al-1Ti-0/15Ta-0/1C
Ni-Cr-Al-Ti-W alloy - Ni-4/13Al-6.5/20.5Cr-0.25/4.75Ti-<4W (at.%)
Ni-Cr-Al-Ti-Y alloy - Inconel MA753 Ni-22Cr-1.6Al-2.7Ti-1.3Y2O3
Ni-Cr-Al-yttria alloy - 48Ni-16Cr-5Al-1Y2O3
Ni-Cr-C alloys - Electrolytic etching
Ni-Cr-Co-C alloys - 25Cr-30Co-0.15C-Ni, Co-25Cr-10Ni-0.15/0.25 C
Ni-Cr-Co-Mo-Ti-Al-Fe-C alloy - Waspaloy Ni-0.06C-19Cr-4Mo-14Co-0.5Fe-1.4Al-3Ti
Ni-Cr-Fe alloy - Alloys with up to 40% Fe - Reveals chromium rich alpha and sigma phases
Ni-Cr-Fe alloy - Electrolytic thinning by Bollmann technique
Ni-Cr-Fe alloys (Inconel) - Electrolytic thinning
Ni-Cr-Fe-Al alloy - Up to 40% Fe and 2% Al - Electrolytic polishing
Ni-Cr-Fe-Mo alloys - Hastelloy X Ni-21Cr-18Fe-9Mo (+C)
Ni-Cr-Fe-Mo-Co-Mn-W-C alloy - Ni-21Cr-19Fe-8.6Mo-2Co-0.6Mn-0.5W-0.1C, Hastelloy X
Ni-Cr-Fe-Mo-Nb alloys - Inconel 718, Ni-19Cr-19Fe-3Mo-5Nb+Al,Ti,C
Ni-Cr-Fe-Nb alloy - Up to 40% Fe and 1% Nb - Electrolytic polishing
Ni-Cr-Fe-Si alloy - Alloys with up to 40% Fe, 1% Si - Electrolytic polishing
Ni-Cr-Mo-Al-C alloy - Ni-15Cr-3/5Mo-7Al-0.2C
Ni-Cr-Mo-C alloy - Ni-15Cr-5Mo-0.2C
Ni-Cr-Mo-Ti-Al-C alloy - Ni-15Cr-0.1/5Mo-2.5/3.5Al-4.5/5.5Ti
Ni-Cr-Mo-W-Al-Ta-C alloy - Ni-6Cr-3Mo-5W-6Al-8Ta-0.1C
Ni-Cr-Ta alloy - 10-12% Cr, 0-15% Ta
Ni-Cr-Ta alloy - 25 wt.% Ta, 10 wt.% Cr
Ni-Cr-Ta-C alloy - 10-12 Cr, 0-15 Ta, 0-1 C
Ni-Cr-Th alloy - 20% Cr, 2% ThO2 - Electrolytic polishing and etching
Ni-Cr-Th alloy - Electrolytic and chemical etching
Ni-Cr-Th alloy - Ni-20Cr-1.35/2.50 ThO2 - Electrolytic thinning and chemical etching
Ni-Cr-Ti alloy - Electrolytic thinning by window technique
Ni-Cu alloy (Monel) - Chemical etching
Ni-Cu alloy - Electrolytic thinning by window technique
Ni-Cu alloys (Monel) - Electrolytic polishing, chemical etching
Ni-Cu alloys - For revealing grain structure
Ni-Fe alloy - 33Ni-67Fe
Ni-Fe alloy - 50Ni-50Fe, 75Ni-25Fe - Shows secondary twins in drawn and rolled material
Ni-Fe alloy - Differences of orientation of martensite plates within prior austenite grains
Ni-Fe alloys (Ni3Fe) - Chemical etching
Ni-Fe alloys - Chemical etching
Ni-Fe alloys - Chemical etching
Ni-Fe alloys - Chemical etching
Ni-Fe alloys - Chemical etching
Ni-Fe alloys, reveals grain boundaries - Chemical ecthing
Ni-Fe, Ni-Mn and Ni-Mo alloys - Chemical etching
Ni-Fe-Cr-Mo alloy - Electrolytic thinning by Bollmann technique
Ni-Fe-Cr-Mo alloys - Hastelloy X.280 Ni-20Fe-22Cr-9Mo-low C
Ni-Fe-Cr-Mo-Ti-Al-C alloy - 901 alloy Ni-0.05C-13Cr-5.6Mo-36.5Fe-0.25Al-2.9Ti
Ni-Fe-Cr-P-B alloy - Metglas 2826A - Fe37-Ni26-Cr14-P17-B6
Ni-Fe-Cr-P-B alloy - Metglas 2826A - Fe37-Ni26-Cr14-P17-B6
Ni-Fe-Cr-Ti alloy - IN 744X, Fe-26.5Cr-6.6Ni, 0.20Ti (+ 0.06 C)
Ni-Fe-Cr-Ti alloys - Chemical etching
Ni-Fe-Cr-Ti alloys - For alloys with Ni-26Fe-35Cr-0.6Ti
Ni-Fe-P-B alloy - Ni40-Fe40-B14-B6 - Electrolytic polishing
Ni-Fe-Ti alloy - Fe-12Ni-0.25Ti
Ni-Fe-Ti alloy - Fe-12Ni-0.25Ti
Ni-Fe-Ti alloy - Fe-6Ti-10-25Ni
Ni-Fe-Ti alloy - Ti4Ni3Fe
Ni-Ga alloy - Alloy with approx. 50 at.% Ga
Ni-Ga alloy - Ni3Ga
Ni-Ge alloys (Ni3Ge single crystal) - Electrolytic polishing
Ni-Mn alloy - Approx. Ni3Mn
Ni-Mn alloy - Electrolytic thinning
Ni-Mn alloys - Dislocation etching
Ni-Mn alloys - Electrolytic polishing
Ni-Mo alloy - Alloy with 16.7 at.% Mo
Ni-Mo alloy - Ni-12/33Mo
Ni-Mo alloy - Ni4Mo
Ni-Mo alloy - Ni4Mo - Electrolytic polishing
Ni-Mo alloy - Ni4Mo - Electrolytic thinning
Ni-Mo alloy - Ni4Mo and Ni3Mo
Ni-Mo alloys - Chemical etching
Ni-Mo steel - Fe-24Ni-4Mo-0.25C
Ni-Mo-Cr-Ti-C alloy - Hastelloy-N, Ni-13Mo-4Cr-2Ti-0.06C
Ni-Mo-Fe alloy - Hastelloy B 65Ni-27Mo-5Fe (+0.3Co, 0.3Si, 0.5Mn, 0.4Cr, 0.3V)
Ni-Nb alloy - Electrolytic thinning for foils
Ni-Nb alloys (Ni-Ni3Nb eutectic) - Electrolytic thinning
Ni-Nb alloys (Ni-Ni3Nb eutectic) - Sample preparation
Ni-Nb alloys - Chemical etching
Ni-Nb-Al alloys - Electrolytic polishing and chemical ecthing
Ni-Si-B glass - Splat cooled alloys
Ni-Si-B system - Chemical etching
Ni-Ta alloy (25 wt.% Ta) - Electrolytic and chemical etching
Ni-Ta alloy (Ni3Ta) - Chemical etching
Ni-Ta alloy - Electrolytic thinning for films
Ni-Ta alloys (low Ta) - Chemical polishing and etching, electrolytic thinning
Ni-Ta alloys - Chemical etching
Ni-Ta-Cr-Al-C eutectic alloy - 69Ni-10Cr-5Al-15Ta-1C
Ni-Ta-Cr-Mn alloy - 57Ni-21Ta-15Cr-7Mn
Ni-Th system - Alloys with 50-70% Ni
Ni-Ti alloy (10 at.% Ti) - Chemical etching
Ni-Ti alloy (NiTi) - Chemical etching
Ni-Ti alloy (NiTi) - Chemical polishing
Ni-Ti alloy (NiTi) - Electrolytic polishing and thinning
Ni-Ti alloy (NiTi) - Electrolytic thinning
Ni-Ti alloys - Chemical etching
Ni-Ti alloys, superalloys - Chemical etching
Ni-Ti-Al alloy - TiNi + 0.05/3.4 at.% Al
Ni-Ti-Al-Si alloys - Chemical etching
Ni-Ti-C alloy - Alloys with 2 wt.% Ti and 0.4 wt.% C
Ni-Ti-Cr-Al alloy - NiTi-2.5 at.% Al-1.5/5 at.% Cr
Ni-V alloy (Ni3V) - Electrolytic thinning and polishing
Ni-V system (Ni3V) - Electrolytic thinning
Ni-W alloy (45% W) - Electrolytic polishing
Ni-W alloys (Ni-26/38% W) - Electrolytic polishing
Ni-W alloys - Electrolytic etching
Ni-Zn alloys (56 wt.% Zn) - Chemical etching
Ni-Zn alloys - Chemical etching
Ni-Zn alloys - Chemical etching
Ni-Zn ferrite (Fe-Ni-O-Zn) - Chemical etching
Ni-Zn ferrite (Fe-Ni-O-Zn) - Ni0.36 x Zn0.64 x Fe2O3
Ni-Zr alloys - Electrolytic etching
Ni-alloys - General macrostructure
Ni-base superalloy - Electrolytic polishing
Ni-base superalloys - Electrolytic polishing
Ni-based superalloys - General macrostructure
Ni-based superalloys, Mar-M200, Udimet-700 - General macrostructure
Ni2B thin film - Metal forming
Ni50Al46Nb4 or Ni40Al39Nb21 alloys - Twin jet polishing mehod
NiAl single crystal specimens - Electrolytic polishing
NiAl specimens and alloys - Electrolytic polishing
NiB thin films - Ketone, cleaning
NiChrome 80-20 etchant - Chemical etching
NiChrome 80-20 etchant - Chemical etching
NiChrome 80-20 etchant - Electrolytic etching
NiCu (30%) single crystal - Thermal forming
NiCu (5%) to NiCu (80%) single crystal wafers - Chemical etching
NiI single crystal - Alcohol removal
NiMn single crystal specimens - Electrolytic etching
NiO (100) cleaved wafers - Thermal etching
NiO - Chemical etching
NiO - Dislocation etching
NiO - Electrolytic etching
NiO single crystal specimens - Physical thinning
NiO specimens - Chemical etching
NiO thin film platelets - Chemical etching
NiS as the natural mineral Millerite - Chemical etching
NiSi thin films deposited on silicon substrates - Ionized gas etching
NiSi2 thin films deposited on silicon wafers - Chemical cleaning
NiSi2 thin films grown on silicon substrates - Chemical etching
NiTi shape memory alloys - General etchant
NiTi single crystal specimens - Chemical etching
NiZn ferrite and Ni ferrite - Chemical etching
Nichrome (20% Cr) - Chemical etching
Nichrome-lanthanum oxide system - Ni-20Cr-1.2/1.6La2O3
Nickel aluminate spinel - Chemical etching
Nickel - Ni-Ag, Ni-Al, Ni-Cr, Ni-Cu, Ni-Fe, and Ni-Ti alloys
Nickel - 80Ni-20Cr and 35Ni-20Cr-45Fe alloys
Nickel - Carbides in Ni-Cr alloys
Nickel - Chemical etching
Nickel - Chemical polishing
Nickel - Chemical polishing
Nickel - Contrast etching
Nickel - Electrolytic etching
Nickel - Electrolytic etching
Nickel - Electrolytic etching
Nickel - Electrolytic etching
Nickel - Electrolytic etching
Nickel - Electrolytic polishing
Nickel - Electrolytic polishing
Nickel - Electrolytic polishing
Nickel - Electrolytic polishing
Nickel - Electrolytic polishing
Nickel - Electrolytic polishing
Nickel - Electrolytic polishing
Nickel - Electrolytic polishing
Nickel - Electrolytic polishing
Nickel - Electrolytic polishing
Nickel - Electrolytic polishing
Nickel - Electrolytic polishing
Nickel - Electrolytic polishing
Nickel - Electrolytic polishing
Nickel - Electrolytic polishing
Nickel - Electrolytic polishing
Nickel - Electrolytic polishing
Nickel - Electrolytic polishing
Nickel - Electrolytic polishing
Nickel - Electrolytic polishing
Nickel - Electrolytic polishing
Nickel - Electrolytic polishing and etching
Nickel - Electrolytic polishing and etching
Nickel - Electrolytic polishing, chemical etching
Nickel - Electrolytic thinning
Nickel - Electrolytic thinning
Nickel - Electrolytic thinning
Nickel - Electrolytic thinning
Nickel - Electrolytic thinning by Bollmann technique
Nickel - Electrolytic thinning by window technique
Nickel - Electrolytic thinning by window technique
Nickel - High alloy Ni, Ni-Cu alloy (Monel), Ni-Al, Ni-Fe alloys
Nickel - Inconel type alloys on Ni-Cr and Ni-Fe-Cr basis
Nickel - Low alloy Ni - Cracks, porosity
Nickel - Ni alloys containing Cr and Fe - Welding joints
Nickel - Ni and Ni base alloys, Bi-Cu alloys, Ni-Cr-Fe alloys
Nickel - Ni and Ni base alloys, Ni-Cr alloys
Nickel - Ni and Ni base alloys, Ni-Cr and Ni-Cr alloys
Nickel - Ni and Ni base alloys, Ni-Cr and Ni-Fe alloys, cast alloys
Nickel - Ni and Ni base alloys, Ni-Cr, Ni-Fe alloys, superalloys of the Nimonic type
Nickel - Ni base superalloys - Gamma precipitates - Ti and Nb microsegregations
Nickel - Ni base superalloys
Nickel - Ni silicides
Nickel - Ni-Al alloys
Nickel - Ni-Al, Mo-Ni, Ni-Ti alloys
Nickel - Ni-Au, Ni-Mo, and Ni-Cr alloys - Micro inhomogenities in superalloys
Nickel - Ni-Cu alloys, Ni base superalloys
Nickel - Ni-Fe and Ni-Al alloys
Nickel - Ni-Fe, Ni-Cu, and Ni-Ag alloys, Ni base superalloys
Nickel - Ni-Zn alloys
Nickel - Ni-Zn-Ag, Ni-Ag-Ni-Cu, and Ni-Al-Mo alloys
Nickel - One of the best electrolyte for universal use
Nickel - Pure types of Ni and alloys with high Ni content, Ni-Ti and Ni-Cu alloys
Nickel - Pysical etching
Nickel - Superalloys - General macrostructure
Nickel alloy - Jet machinning
Nickel alloys - Electrolytic polishing
Nickel alloys - Electrolytic polishing
Nickel and Ni-Co alloys - Electrolytic polishing
Nickel and nickel alloys - Electrolytic polishing
Nickel and nickel alloys - Electrolytic polishing
Nickel and nickel alloys - Electrolytic polishing
Nickel and nickel alloys - Electrolytic polishing
Nickel and nickel alloys - Electrolytic polishing
Nickel and nickel alloys - Electrolytic polishing
Nickel and nickel alloys - For revealing cracks, porosity, dendritic patterns in cast alloys
Nickel and nickel alloys - Ni-Cr and Ni-Cr-Fe alloys
Nickel and nickel alloys - Reveals cracks, porosity, etc.
Nickel and nickel-copper alloys (Ni-Cu) - For Monel K-500 alloy
Nickel and nickel-copper alloys (Ni-Cu) - For revealing grain boundaries
Nickel and nickel-copper alloys (Ni-Cu) - Microscopic examination of grain boundaries and general structure
Nickel base alloy - Electrolytic thinning by PTFE holder
Nickel base superalloy - Selective phase contrasting
Nickel base superalloy GMR 235 - Chemical etching
Nickel base superalloy GTD111 - Chemical etching
Nickel ferrite (Ni-Fe-O) - Chemical etching
Nickel oxide (NiO) - Chemical etching
Nickel oxide (NiO) - Chemical thinning
Nickel phosphorus alloys (Ni-P) - Electrolytic and chemical polishing
Nickel phosphorus glass (Ni-P) - Ni80P20
Nickel plating
Nickel single crystal - Electrolytic polishing
Nickel specimens - Chemical etching
Nickel specimens - Chemical etching
Nickel specimens - Chemical etching
Nickel specimens - Chemical etching
Nickel specimens - Electrolytic polishing
Nickel specimens TD - Thorium deposited nickel - Etch for grain boundary
Nickel specimens and nickel alloys - Electrolytic polishing
Nickel superalloy 718 - Chemical etching
Nickel superalloy 718 - Chemical etching
Nickel superalloy 718 - Chemical etching
Nickel superalloy 718 - Electrolytic etching
Nickel superalloy 718 - Electrolytic etching
Nickel superalloy 718 - Electrolytic etching
Nickel superalloy 718 - Electrolytic etching
Nickel superalloys - Chemical etching - General macrostructure
Nickel superalloys - Chemical etching - General macrostructure
Nickel superalloys - Etching for gamma prime in superalloys
Nickel superalloys - Grain size and texture are well revealed - Freckles are less easily seen
Nickel superalloys - Macrostructure clearly revealed
Nickel superalloys - Production of thin foils for electron microscopy
Nickel superalloys - Production of thin foils for electron microscopy
Nickel superalloys - Production of thin foils for electron microscopy
Nickel superalloys - Production of thin foils for electron microscopy
Nickel superalloys - Production of thin foils for electron microscopy
Nickel superalloys - Production of thin foils for electron microscopy
Nickel superalloys - Production of thin foils for electron microscopy
Nickel superalloys - Production of thin foils for electron microscopy
Nickel superalloys - Production of thin foils for electron microscopy
Nickel(CP, HP) - Dislocation etching
Nickel-Ni base superalloys - Especially suitable for Hastelloy types
Nicrofer alloy - Electrolytic polishing
Nimonic 105 - Ni-0.14C-0.3Fe-14.4Cr-1.3Ti-4.7Al-20Co-5Mo
Nimonic 115 alloy - Ni-15Cr-15Co-4Ti-3.5Mo-5Al
Nimonic 80 alloy - Ni-21Cr-2.7Ti-1.6Al-1.5Fe-2Co-0.8Si-0.4Mn-0.2Cu-0.1C
Nimonic 80A - Electrolytic thinning, electrolytic polishing
Nimonic 80A - Ni-20Cr-1.3Al-2.3Ti
Nimonic PE 16 - Fe-43.5Ni-16.5Cr-1.2Ti-3.2Mo-1.2Al
Nimonic alloys - Macro defects in the Nimonic alloys
Nimonic alloys - Macro defects in the Nimonic alloys
Nimonic alloys - Nimonic 108, 109, 115, 120, EPK 55, Nimonic PK 33 and PK 50
Nimonic alloys - Nimonic 263
Nimonic alloys - Nimonic 75, 80A, 90, 93, 105, 108, 109, 115, 120, EPK 55, and EPK 57. Nimocast alloys
Nimonic alloys - Nimonic 901
Nimonic alloys - Nimonic PE 7, PE 11, PE 16, Nimonic 901
Nimonic alloys - Nimonic PK 31
Nimonic alloys - Nimonic PK 31, Nimonic EPK 57
Nimonic alloys - Nimonic PK 31, Nimonic EPK 57
Nimonic alloys - Nimonic PK 33, PK 50, Nimonic 901
Nimonic alloys - Nimonic alloys 75, 80A, 90, 93, 105
Nimonic, Ni-Cr-Co alloys, Ni-Cr-Co-Mo alloys - General macrostructure
Nimonic, Ni-Cr-Co alloys, Ni-Cr-Co-Mo alloys - General macrostructure
Nital (10%) - Nickel superalloy 718 - Electrolytic etching
Nital - Fe-Ni (5%)-O (15%) specimens - Chemical etching
Nitinol - NiTi alloys
Oxide ceramics - NiO
Oxide dispersed Ni-Cr-Al-Fe alloy - Ni-16Cr-4.2Al-0.2Fe-0.8/1.0Y2O3-1.6/2.0Al2O3 +C,N
Oxide dispersion hardened MA6000L alloy - Ni-14Cr-4.6Al-4W-2.3Ti-2.1Ta-2Mo-0.75Y-0.6O2-0.2Fe-0.2N-0.07C-0.07Zr (+B)
Precision No. 2 etchant - Ni alloys - Chemical etching
Pure Ni - Chemical etching
Pure Ni - Chemical polishing
Pure Ni, Ni-Co alloys - Chemical polishing
Pure Ni, Ni-Zn-Ag, Ni-Ag, Ni-Cu and Ni-Al-Mo alloys - Chemical etching
Pure Ni, superalloys, Ni-Cr and Ni-Fe alloys - Chemical etching
RNi6B2 specimens - Chemical etching
Rene 125 alloy - Ni-10Co-8.9Cr-7.0W-4.75AL-3.8Ta-2.5Ti-2.0Mo-1.5Hf-0.11C (+ 0.05Zr, 0.01B)
Rene 80 alloy - Chemical etching
Rene 80 alloy - Ni-14Cr-4Mo-5Ti-3Al-9Co-4W-0.2C (+ Zr, B)
Rene 95 alloy - 62.2Ni-12.8Cr-8.0Co-3.6Al-3.7Mo-3.5Nb-3.5W-2.6Ti-0.8C by weight
Rene 95 alloy - Ni-01.6C-14Cr-8Co-3.5Mo-2.5W-2.5Ti-3.4Al-3.6Nb
Rene 95 alloy powder - Chemical etching
Rene 95 nickel alloy - Chemical etching
SM-200 nickel alloy - Chemical etching
Segregation in speralloys - Chemical and elctrolytic etching
Shape memory alloys - Chemical etching
Solder paste alloys - NiTi alloys
Superalloy 713LC - Ni-11.7Cr-4.5Mo-6Al-0.75Ti-2Nb(+Ta) (+0.06C)
Superalloy B-1900 - 65Ni-10Co-8Cr-6Mo-6Al-4Ta-1Ti-0.1C-0.1Zr-0.015B
Superalloy In 100 - 60Ni-15Co-10Cr-3Mo-5.5Al-5Ti-1V-0.18C-0.06Zr-0.014B
Superalloy MAR200 - 60Ni-10Co-9Cr-12.5W-5Al-2Ti-1Nb-0.15C-0.05Zr-0.015C
Superalloy MAR200 - Chemical etching
Superalloy MAR200 - Plastic deformation can be revealed by polish-etch-electro polish technique
Superalloy Udimet 700 - 56Ni-17Co-15Cr-5Mo-4Al-3Ti-0.07C
Superalloys - Electrolytic polishing
Superalloys - Electrolytic polishing
Superalloys - Etches gamma phase, carbides, and grain boundaries
Superalloys - Etches gamma phase, carbides, grain-contrast etchant
Superalloys, Hastelloy A type - Chemical etching
Surface layers on Ni-base alloys, plasma coatings - Chemical etching
T.D. Ni-Cr alloy - 20% Cr-2% ThO2 - Electrolytic polishing and etching
TD-Ni, DS-NiCr, Inconel MA-754, TD-NiCrAl and DST-NiCrAl - Chemical etching
TD-NiCr alloy - Heat tint etching
TD-Nickel - Electrolytic etching
TD-nickel, TD-NiCrAl, Inconel, MA-754 - General macrostructure
TRW-NASA VIA alloy - Ni-6Cr-2Mo-1Ti-5.5Al-9Ta-6W-7.5Co-0.5Hf-0.4Re-0.15C (+B, Zr)
Udimet 500 alloy - Ni-15/20Cr-13/20Co-3/5Mo-2.5/3.25Al-0/4Fe
Udimet 700 - Chemical etching
Udimet 700 - Chemical etching
Udimet 700 - Electrolytic polishing, chemical etching
Udimet 700 - Stain etch for inclusions
Udimet 700 alloy - Ni-18.5Co-13Cr-3.5Ti-4.3Al-5.3Mo-0.08C-0.03B
Udimet 700 and Rene 41 - Chemical etching
Vilella's etchant - Nickel superalloys - Production of thin foils for electron microscopy
Walker's etchant - Ni alloys
Walker's etchant - Rene 95 alloy
Walker's etchant - Rene 95 alloy - Chemical ecthing
Walker's etchant - Rene 95 alloy - Chemical etching
Waspaloy - 59.2Ni-13.2Co-18.8Cr-4.1Mo-1.2Al-3.0Ti-0.04C by weight
Waspaloy - Twin jet polishing mehod
Waterless Kallings's etchant - Nickel superalloy 718 - Chemical etching
Wrought Fe-Ni-Cr heat resisting alloy - U-700 (AISI 687) - General structure; grain boundaries
Wrought Fe-Ni-Cr heat resisting alloys - Inconel 600 and 601 - General structure
Wrought Fe-Ni-Cr heat resisting alloys - Inconel 600 and 601 - General structure; carbide particles
Wrought Fe-Ni-Cr heat resisting alloys - Inconel 600 and 601 - General structure; grain boundaries; carbide
Wrought Fe-Ni-Cr heat resisting alloys - Inconel 600 and 601, excellent for revealing carbide particles
Wrought Fe-Ni-Cr heat resisting alloys - Inconel 600 and 601- Grain boundary contrast
Wrought Fe-Ni-Cr heat resisting alloys - Inconel 625
Wrought Fe-Ni-Cr heat resisting alloys - Inconel 625 - Grain boundaries
Wrought Fe-Ni-Cr heat resisting alloys - Inconel 625 - Grain boundary films
Wrought Fe-Ni-Cr heat resisting alloys - Inconel 625, general structure
Wrought Fe-Ni-Cr heat resisting alloys - Inconel 625, general structure; grain boundaries
Wrought Fe-Ni-Cr heat resisting alloys - Inconel 706 and alloy 718
Wrought Fe-Ni-Cr heat resisting alloys - Inconel 706 and alloy 718 - General structure; microsegregation
Wrought Fe-Ni-Cr heat resisting alloys - Inconel 706 and alloy 718 - General structure; precipitate phases
Wrought Fe-Ni-Cr heat resisting alloys - Inconel 706 and alloy 718 - Good for general structure and phase outline; grain boundaries
Wrought Fe-Ni-Cr heat resisting alloys - Inconel 706 and alloy 718 - Grain boundary films
Wrought Fe-Ni-Cr heat resisting alloys - Inconel X-750 (AISI 688) - Excellent for showing details of overaged gamma prime
Wrought Fe-Ni-Cr heat resisting alloys - Inconel X-750 (AISI 688) - Good for revealing grain boundaries and carbide particles
Wrought Fe-Ni-Cr heat resisting alloys - Inconel X-750 (AISI 688), general structure
Wrought Fe-Ni-Cr heat resisting alloys - Inconel X-750 (AISI 688), grain boundaries; carbide
Wrought Fe-Ni-Cr heat resisting alloys - Inconel X-750 (AISI 688)- General structure; microsegregation
Wrought Fe-Ni-Cr heat resisting alloys - Waspaloy (AISI 685) - General structure
Wrought Fe-Ni-Cr heat resisting alloys - Waspaloy (AISI 685) - General structure
Wrought Fe-Ni-Cr heat resisting alloys - Waspaloy (AISI 685) - General structure
Yittria dispersed Nichrome - (Cr-Ni-O-Y)-Ni-20Cr-0.2/1.1Y2O3
ZIP's etchant - Inconel 617 - Chemical etching