31CrMoV9 Steel

Steel name: 31CrMoV9
Table No.: 1729
DIN designation: 31CrMoV9
Mat.No. (Wr.Nr.) designation: 1.8519
AISI/SAE designation: 31CrMoV9
EN designation: 31CrMoV9
UNI designation: 31CrMoV9
AFNOR designation: 31CrMoV9
Chemical composition in weight %: 0.27-0.34% C, max. 0.30% Si, 0.40-0.70% Mn, max. 0.025% P, max. 0.035% S, 2.30-2.70% Cr, 0.15-0.25% Mo, 0.10-0.20% V
Steel group: Nitriding steels
Applications: No data
Comment: Ac1=760 C, Ac3=820 C, Ms=350 C, Mf=130 C.
Reference: Not shown in this demo version.

Heat Treatment
Quenching: 850-880 C/polymer
Tempering: 580-700/air

Hardenability Table

Price: 20.00 US $
Buy Online Hardenability Table

Other Steel Data links:
Carbides in Steel
CCT & TTT Diagrams of Steels
Etchants Database
Hardenability Calculating Service
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2017 by Steel Data. All Rights Reserved.