Home
Underdeveloped Photoresist
Material Name: Photoresist
Record No.: 153
Primary Chemical Element in Material: No data
Sample Type: Wafer
Uses: Etching
Etchant Name: None
Etching Method: No data
Etchant (Electrolyte) Composition: No data
Procedure (Condition): No data
Note: No data
Reference: Owen Cherry, Fabrication of an Atom Chip for Rydberg Atom-Metal SurfaceInteraction Studies, MSc Thesis, University of Waterloo, Ontario, 2007, p. 106.

Figure 1: Microscope image of underdeveloped lift-off photoresist (Futurrex NR1-3000PY). The resist
is continuous between the wires.